| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Unnotched | 3.47 - 8.01 J/cm | 6.50 - 15.0 ft-lb/in | Average value: 5.06 J/cm Grade Count:16 |
|
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
|
|||
| Izod Impact, Unnotched | 2.67 - 8.01 J/cm | 5.00 - 15.0 ft-lb/in | Average value: 4.50 J/cm Grade Count:7 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| Izod Impact, Unnotched | 3.74 - 8.01 J/cm | 7.00 - 15.0 ft-lb/in | Average value: 5.49 J/cm Grade Count:7 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a..
|
|||
| Izod Impact, Unnotched | 0.747 - 8.01 J/cm | 1.40 - 15.0 ft-lb/in | Average value: 5.35 J/cm Grade Count:40 |
|
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
|
|||
| Izod Impact, Unnotched | 1.60 - 8.00 J/cm | 3.00 - 15.0 ft-lb/in | Average value: 4.41 J/cm Grade Count:11 |
|
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
|
|||
| Izod Impact, Unnotched | 6.14 - 8.01 J/cm | 11.5 - 15.0 ft-lb/in | Average value: 7.14 J/cm Grade Count:4 |
|
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
|
|||
| Izod Impact, Unnotched | 0.854 - 8.00 J/cm | 1.60 - 15.0 ft-lb/in | Average value: 4.97 J/cm Grade Count:42 |
|
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
|
|||