| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Unnotched |
15.48
J/cm <br>@Temperature 23.0 °C
|
29.00
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D 4812 |
|
SABIC Innovative Plastics LNP Lubricomp DP003F PC
LNP LUBRICOMP* DP003F is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the..
|
|||
| Izod Impact, Unnotched |
15.48
J/cm <br>@Temperature 23.0 °C
|
29.00
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D 4812 |
|
SABIC Innovative Plastics LNP Lubricomp DP003F PC (Asia Pacific)
LNP LUBRICOMP* DP003F is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the..
|
|||
| Izod Impact, Unnotched | 15.48 J/cm | 29.00 ft-lb/in | ASTM D4812 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK
LNP* LUBRICOMP* LL004C is a compound based on Polyetheretherketone resin containing 20% PTFE. Added features of this material include: Wear Resistant, Clean Compounding System.
|
|||
| Izod Impact, Unnotched | 15.48 J/cm | 29.00 ft-lb/in | ASTM D4812 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK (Asia Pacific)
LNP* Lubricomp* LL004C is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated, Clean Compounding System.
|
|||
| Izod Impact, Unnotched | 15.48 J/cm | 29.00 ft-lb/in | ASTM D4812 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK
LNP* LUBRICOMP* LL004E is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
|
|||
| Izod Impact, Unnotched | 15.48 J/cm | 29.00 ft-lb/in | ASTM D4812 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK (Asia Pacific)
LNP* Lubricomp* LL004E is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Izod Impact, Unnotched |
15.48
J/cm <br>@Temperature 23.0 °C
|
29.00
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D 4812 |
|
SABIC Innovative Plastics Ultem 1100EF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Unnotched |
15.48
J/cm <br>@Temperature 23.0 °C
|
29.00
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D 4812 |
|
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Unnotched |
15.48
J/cm <br>@Temperature 23.0 °C
|
29.00
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D 4812 |
|
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region..
|
|||
| Izod Impact, Unnotched | 15.48 J/cm | 29.00 ft-lb/in | ASTM D4812 |
|
SABIC Innovative Plastics LNP STAT-KON DD0009E PC (Asia Pacific)
LNP* Stat-kon* DD0009E is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Izod Impact, Unnotched | 15.48 J/cm | 29.00 ft-lb/in | ASTM D4812 |
|
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA 11 (Asia Pacific)
LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing Glass Bead.
|
|||
| Izod Impact, Unnotched | 15.48 J/cm | 29.00 ft-lb/in | ASTM D4812 |
|
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA11
LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing 30% Glass Bead.
|
|||
| Izod Impact, Unnotched |
15.48
J/cm <br>@Temperature 23.0 °C
|
29.00
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D 4812 |
|
SABIC Innovative Plastics LNP Stat-kon MD000IU PP
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..
|
|||
| Izod Impact, Unnotched |
15.48
J/cm <br>@Temperature 23.0 °C
|
29.00
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D 4812 |
|
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific)
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..
|
|||