Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 18.0 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.490 - 9.61 J/cm
0.919 - 18.0 ft-lb/in
Average value: 5.05 J/cm Grade Count:13
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Izod Impact, Unnotched 3.20 - 9.61 J/cm
6.00 - 18.0 ft-lb/in
Average value: 5.96 J/cm Grade Count:8
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Izod Impact, Unnotched 2.67 - 9.60 J/cm
5.00 - 18.0 ft-lb/in
Average value: 4.99 J/cm Grade Count:18
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Izod Impact, Unnotched 2.50 - 9.61 J/cm
4.68 - 18.0 ft-lb/in
Average value: 5.96 J/cm Grade Count:23
Overview of materials for Polyarylamide, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values..
Izod Impact, Unnotched 8.01 - 9.61 J/cm
15.0 - 18.0 ft-lb/in
Average value: 8.54 J/cm Grade Count:3
Overview of materials for Nylon 6, Stainless Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o..
Izod Impact, Unnotched 3.20 - 9.61 J/cm
6.00 - 18.0 ft-lb/in
Average value: 6.80 J/cm Grade Count:26
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Izod Impact, Unnotched 0.883 - 9.60 J/cm
1.65 - 18.0 ft-lb/in
Average value: 5.64 J/cm Grade Count:10
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Izod Impact, Unnotched 6.40 - 9.60 J/cm

@Temperature -40.0 - -40.0 °C
12.0 - 18.0 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 8.00 J/cm Grade Count:2
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Izod Impact, Unnotched 0.932 - 9.60 J/cm
1.75 - 18.0 ft-lb/in
Average value: 6.00 J/cm Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
Izod Impact, Unnotched 1.60 - 9.61 J/cm
3.00 - 18.0 ft-lb/in
Average value: 6.63 J/cm Grade Count:11
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..
Copyright © lookpolymers.com All Rights Reserved