Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 2.50 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.50 J/cm
4.68 ft-lb/in
ASTM D256
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral  (discontinued **)
Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical..
Izod Impact, Unnotched 2.50 - 9.61 J/cm
4.68 - 18.0 ft-lb/in
Average value: 5.96 J/cm Grade Count:23
Overview of materials for Polyarylamide, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values..
Izod Impact, Unnotched 2.50 J/cm

@Temperature -40.0 °C
4.68 ft-lb/in

@Temperature -40.0 °F
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin
Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..
Izod Impact, Unnotched 2.50 J/cm
4.68 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP IBI16 PA 6/12
LNP LUBRICOMP* IBI16 is a compound based on Nylon 6/12 resin containing 30% Glass Bead, 2% Silicone. Added features of this material include: Wear Resistant.
Izod Impact, Unnotched 2.50 J/cm
4.68 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® CS815 PBT+PET
15% glass reinforced PBT+PET. Improved heat aged color stability, high surface gloss. Oven knobs and handles, kickplates, trim.
Izod Impact, Unnotched 2.50 J/cm
4.68 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS
LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic.
Izod Impact, Unnotched 2.50 J/cm
4.68 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific)
LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat.
Izod Impact, Unnotched 2.50 J/cm
4.68 ft-lb/in
ISO 180
Solvay Specialty Polymers Primef® 4002 40% GF PPS, High Fluidity Grade  (discontinued **)
Used for injection molding of high performance parts.
Izod Impact, Unnotched 2.50 J/cm

@Temperature -40.0 °C
4.68 ft-lb/in

@Temperature -40.0 °F
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin
Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..
Izod Impact, Unnotched 2.50 - 8.27 J/cm
4.68 - 15.5 ft-lb/in
Average value: 5.56 J/cm Grade Count:15
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Unnotched 2.50 J/cm
4.68 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)  (discontinued **
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Copyright © lookpolymers.com All Rights Reserved