Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.20 J/cm | 6.00 ft-lb/in | ASTM D256 |
Network Polymers NPP 30-1200 TF20 Description: 20% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Unnotched | 3.20 - 5340 J/cm | 6.00 - 10000 ft-lb/in | Average value: 8.10 J/cm Grade Count:7 |
Overview of materials for Polycarbonate/Polysulfone Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Unnotched | 3.20 - 60.0 J/cm | 6.00 - 112 ft-lb/in | Average value: 8.89 J/cm Grade Count:34 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at.. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® BR111BL is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical proper.. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® ABS GF10 FR 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, I.. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal.. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF50 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS LG GF10 UV BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAdditive: UV StabilizerFeatures: Good UV Resistance and Low GlassAppearance: BlackInform.. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Temperature -30.0 °C |
5.99 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Temperature -40.0 °C |
5.99 ft-lb/in @Temperature -40.0 °F |
ASTM D4812 |
Eastman Eastar EN076 Copolyester Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o.. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Adell ER-14 Homopolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester, TP (Asia Pacific) LNP* THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Mineral, Glass Fiber. Added features of this material include: Flame Retardant. |