Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 6.40 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP COLORCOMP PX99848 PA 6 (Asia Pacific)
LNP* Colorcomp* PX99848 is a compound based on Nylon 6 resin containing Unfilled Custom Color.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC (Asia Pacific)
LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Ineos H12Z-02 Polypropylene Homopolymer, Antistatic and Nucleated
A nucleated and antistated polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications that require superior mold release pro..
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D256A
LyondellBasell Higlass SB224-2 Polypropylene Copolymer, 20% Glass Fiber
Key Features: conventional melt flow, medium modulus, chemically coupled, glass fiber-reinforced polypropylene copolymer, high impact strength, moderate rigidity, good processabilityApplications: of..
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer
LNP LUBRICOMP* KL004 is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Asia Pacific)
LNP Lubricomp* KL004 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* Fu..
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical..
Izod Impact, Unnotched 6.40 J/cm

@Thickness 3.18 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
Izod Impact, Unnotched 6.40 J/cm

@Thickness 3.18 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un..
Izod Impact, Unnotched 6.40 J/cm

@Thickness 3.18 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber
Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low ..
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 508R PBT+PC
30% GR PBT+PC. Excellent mechanical and thermal performance. Non-FR. Reduced warpage characteristics. Applications same as VALOX 420R.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 830 PBT
30% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 830 PBT (Asia Pacific)
30% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 865 PBT+PET
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer
LNP* THERMOCOMP* KF006XXC is a compound based on Acetal Copolymer resin containing 30% Glass Fiber.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific)
LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear (Asia Pacific)
LNP* Thermocomp* OC006 is a compound based on PPS - Linear resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 6.40 J/cm

@Thickness 3.18 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur..
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON OE006 PPS - Linear
LNP* STAT-KON* OE006 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP EF006H PEI
LNP* Thermocomp* EF006H is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features include: Healthcare.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP EF006H PEI (Asia Pacific)
LNP* Thermocomp* EF006H is a compound based on Polyetherimide resin containing Glass Fiber.
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear
LNP* THERMOCOMP* OC006 is a compound based on PPS-Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 6.40 J/cm

@Temperature 23.0 °C
12.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp JX89569 PES (Asia Pacific)
LNP* THERMOCOMP* JX89569 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Unnotched 6.40 - 9.60 J/cm

@Temperature -40.0 - -40.0 °C
12.0 - 18.0 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 8.00 J/cm Grade Count:2
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4-200NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low mainten..
Copyright © lookpolymers.com All Rights Reserved