Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 6.50 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.47 J/cm

@Thickness 3.18 mm
6.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Lubricomp® OFL-4536 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Izod Impact, Unnotched 3.47 J/cm - NB
6.50 ft-lb/in - NB
Average value: 6.24 J/cm Grade Count:9
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Izod Impact, Unnotched 3.47 J/cm

@Temperature 23.0 °C
6.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp KZL34 POM
LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas..
Izod Impact, Unnotched 3.47 J/cm
6.50 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 (Asia Pacific)
LNP* Lubricomp* RP004 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 3.47 J/cm
6.50 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS
LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability.
Izod Impact, Unnotched 3.47 J/cm

@Thickness 3.17 mm
6.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® PC NCF15 FR 15% Nickel-Coated Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation ..
Izod Impact, Unnotched 3.47 J/cm
6.50 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DE0021E PC
LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding, Flame Retardant, Electrically Conductive.
Izod Impact, Unnotched 3.47 J/cm
6.50 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific)
LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding.
Izod Impact, Unnotched 3.47 J/cm

@Thickness 3.17 mm
6.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® ABS E GM15 LE 15% Glass Filled
Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 3.47 J/cm

@Temperature 23.0 °C
6.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Stat-kon NX03602 PC+ABS
LNP STAT-KON* NX03602 is a compound based on PC+ABS Blend resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supplied by ..
Izod Impact, Unnotched 3.47 J/cm

@Temperature 23.0 °C
6.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Stat-kon NX03602 PC+ABS (Asia Pacific)
LNP* STAT-KON* NX03602 is a compound based on PC+ABS Blend resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supplied by..
Izod Impact, Unnotched 3.47 J/cm

@Thickness 3.17 mm
6.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PP GF10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 3.47 J/cm

@Temperature 23.0 °C
6.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6
LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC..
Izod Impact, Unnotched 3.47 J/cm

@Temperature 23.0 °C
6.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6 (Asia Pacific)
LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC..
Izod Impact, Unnotched 3.47 J/cm
6.50 ft-lb/in
ASTM D256
A. Schulman ComAlloy Comtuf® 103 Polypropylene, Glass Reinforced, Chemically Coupled, Impact Modified
Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int..
Izod Impact, Unnotched 3.47 - 5340 J/cm
6.50 - 10000 ft-lb/in
Average value: 6.69 J/cm Grade Count:47
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Unnotched 3.47 - 7.47 J/cm
6.50 - 14.0 ft-lb/in
Average value: 5.62 J/cm Grade Count:6
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..
Copyright © lookpolymers.com All Rights Reserved