| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Unnotched | 3.74 J/cm - NB | 7.00 ft-lb/in - NB | Average value: 5.76 J/cm Grade Count:17 |
|
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
|
|||
| Izod Impact, Unnotched |
3.74
J/cm @Thickness 3.17 mm |
7.00
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Techmer ES HiFill® HDPE TM20 20% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D4812 |
|
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT
Information provided by A. Schulman.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D4812 |
|
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D4812 |
|
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
|
|||
| Izod Impact, Unnotched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D4812 |
|
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
|
|||
| Izod Impact, Unnotched | 3.74 - 6.94 J/cm | 7.00 - 13.0 ft-lb/in | Average value: 4.68 J/cm Grade Count:19 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
|
|||