Polymer Property : Izod Impact, Unnotched = 9.61 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.490 - 9.61 J/cm
0.919 - 18.0 ft-lb/in
Average value: 5.05 J/cm Grade Count:13
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Izod Impact, Unnotched 3.20 - 9.61 J/cm
6.00 - 18.0 ft-lb/in
Average value: 5.96 J/cm Grade Count:8
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Izod Impact, Unnotched 2.50 - 9.61 J/cm
4.68 - 18.0 ft-lb/in
Average value: 5.96 J/cm Grade Count:23
Overview of materials for Polyarylamide, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values..
Izod Impact, Unnotched 8.01 - 9.61 J/cm
15.0 - 18.0 ft-lb/in
Average value: 8.54 J/cm Grade Count:3
Overview of materials for Nylon 6, Stainless Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o..
Izod Impact, Unnotched 3.20 - 9.61 J/cm
6.00 - 18.0 ft-lb/in
Average value: 6.80 J/cm Grade Count:26
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Izod Impact, Unnotched 1.60 - 9.61 J/cm
3.00 - 18.0 ft-lb/in
Average value: 6.63 J/cm Grade Count:11
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..