Mechanical Properties Metric English Comments
Tensile Strength at Break 180 MPa
26100 psi
ISO 527
Nilit FRIANYL B63 W-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Strength at Break 180 MPa
26100 psi
ISO 527
Nilit FRIANYL B63 GV35 Nylon 6 for injection molding, 35% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Strength at Break 180 MPa
26100 psi
ISO 527
Nilit FRIANYL B63 HH-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced
Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Strength at Break 180 MPa
26100 psi
ISO 527
Nilit FRIANYL C73 GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced
Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Strength at Break 180 MPa
26100 psi
ISO 527
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced
Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Strength at Break 180 MPa
26100 psi
ISO 527-1/-2
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance
Tensile Strength at Break 180 MPa
26100 psi
ISO 527-1/-2
Lanxess Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance
Tensile Strength at Break 180 MPa
26100 psi
d.a.m.; ISO 527-1, -2; 5 mm/min
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS.
Tensile Strength at Break 180 MPa
26100 psi
5 mm/min; ISO 527
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
Tensile Strength at Break 180 MPa
26100 psi
5 mm/min; ISO 527
SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be..
Tensile Strength at Break 180 MPa
26100 psi
5 mm/min; ISO 527
SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
Tensile Strength at Break 180 MPa
26100 psi
5 mm/min; ISO 527
SABIC Innovative Plastics Ultem 2410F PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). UL94 V0 and 5VA listing. US FDA and European Food contact approved. Effective June, 2007 this grade will no longer be supported with b..
Tensile Strength at Break 180 MPa
26100 psi
ISO 527
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66
LNP STAT-KON* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ..
Tensile Strength at Break 180 MPa
26100 psi
ISO 527-93
Wellman Wellamid® GF43-66 XE-NBK1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman.
Tensile Strength at Break 180 MPa
26100 psi
ISO 527-93
Wellman Wellamid® GFX1872-N1 (PTFE) Nylon 66, 33% Glass Reinforced, Lubricated
All information provided by Wellman Engineered Resins.
Tensile Strength at Break 180 MPa
26100 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BG-30 FC PA6-GF30
Product description: Grilon BG-30 FC is a heat stabilised PA6 injection moulding grade with 30% glass fibres. Grilon BG-30 FC has the following important properties: High stiffnessExcellent surface ..
Tensile Strength at Break 180 MPa
26100 psi
ISO 527-1/-2
DSM Stanyl® TS256F8 Nylon 46-40% Glass Reinforced (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Strength at Break 180 MPa
26100 psi
5 mm/min; ISO 527
CP-Polymer-Technik Wellamid® 6600 GV 30 HWCP 30% Glass Fiber Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Strength at Break 180 MPa
26100 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® HT2VZ-33H PA6T/66-GF33
Product description: Grivory HT2VZ-33H is a 33% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT2VZ-33H is an injecti..
Tensile Strength at Break 180 MPa
26100 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® LV-65H SST nat PA12-GF65
Product description: Grilamid LV-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the foll..
Tensile Strength at Break 180 MPa
26100 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® XE 5026 (BG-30 H) PA6-GF30
Product description: Grilon B XE 5026 (BG-30 H) black 9922 is a high heat stabilized, 30% glass fiber reinforced PA6- Injection molding grade with modified flowability. Grilon B XE 5026 (BG-30 H) bl..
Tensile Strength at Break 180 MPa
26100 psi
5 mm/min; ISO 527
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded
AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Tensile Strength at Break 180 MPa
26100 psi
5 mm/min; ISO 527
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded
Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Tensile Strength at Break 180 MPa
26100 psi
5 mm/min; ISO 527
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded
Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Tensile Strength at Break 180 MPa
26100 psi
ISO 527-1/-2
Lanxess Durethan® BKV 35 H2.0 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: automotive structures
Tensile Strength at Break 180 MPa
26100 psi
ISO 527-1/-2
Lanxess Durethan® BKV 30 W1 000000 Nylon 6, 30% Glass Fiber
PA 6, Injection molding grade, 30% glass fibers, weather stabilized