Polymer Property : Tensile Strength at Break = 20.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.6 - 20.7 MPa
2700 - 3000 psi
ITW Plexus Plexusâ„¢ AO420 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive , high toughness.Information provided by Illinois Tool Works.
Tensile Strength at Break 17.2 - 20.7 MPa
2500 - 3000 psi
ITW Plexus Plexusâ„¢ MA556 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Information provided by Illinois Tool Works..
Tensile Strength at Break 17.2 - 20.7 MPa
2500 - 3000 psi
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois ..
Tensile Strength at Break 18.6 - 20.7 MPa
2700 - 3000 psi
ITW Plexus Plexusâ„¢ MA920 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, short open time.Information provided by Illinois Tool Works.
Tensile Strength at Break 17.2 - 20.7 MPa
2500 - 3000 psi
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works.
Tensile Strength at Break 13.8 - 20.7 MPa
2000 - 3000 psi
Abatron AboCast 7802-1/AboCure 50-3 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, ..
Tensile Strength at Break 13.8 - 20.7 MPa
2000 - 3000 psi
Abatron AboCast 7802-1/AboCure 7804-4 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia..