| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 17.2 MPa | 2490 psi | Type IV, 510 mm/min; ASTM D638 |
|
PolyOne Geon™ Vinyl Flexible XV3853 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | Type IV, 510 mm/min; ASTM D638 |
|
PolyOne Geon™ HC 2175G Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2175G is a 75 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2175G can be used for extrusion and injection molding healthcare applicatio..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | ASTM D3759 |
|
3M 21825 Industrial Polyethylene Temporary Surface Protection Tape
3M™ Industrial Polyethylene Temporary Surface Protection Tape 21825 is a very low adhesion temporary protection tape designed for a variety of surface protection applications.Information provided b..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | ASTM D3759 |
|
3M 3W25X Protective UV Tape
3M™ Protective UV Tape 3W25X is a black and white co-extruded polyethylene tape for temporary indoor and outdoor protection of many metals, plastics and glass.Information provided by 3M
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | ASTM D3759 |
|
3M 3W29X Protective UV Tape
3M™ Protective UV Tape 3W29X is a black and white co-extruded polyethylene tape for temporary indoor and outdoor protection of many metals, plastics and glass.Information provided by 3M
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | ASTM D3759 |
|
3M 41826 Industrial Polyethylene Temporary Surface Protection Tape
3M™ Industrial Polyethylene Temporary Surface Protection Tape 41826 is a very low adhesion temporary protection tape designed for a variety of surface protection applications.Information provided b..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ 1000-19 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ 1000-58 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ 3632-156 Translucent Film
2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ 3632-43 Translucent Film
2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre..
|
|||
| Tensile Strength at Break | >= 17.2 MPa | >= 2490 psi | |
|
3M Scotchcal™ 8000-15 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ ElectroCut™ 7125-103 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ ElectroCut™ 7125-177 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ ElectroCut™ 7125-86 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ ElectroCut™ 7125-99 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ ElectroCut™ 7725-10 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ ElectroCut™ 7725-103 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ ElectroCut™ 7725-176 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ ElectroCut™ 7725-54 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ ElectroCut™ 7725-63 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Tensile Strength at Break | >= 17.2 MPa | >= 2490 psi | |
|
3M Scotchcal™ IJ3650-114 Graphic Film
2-mil, opaque white and transparent film; Pressure-sensitive adhesive; Permanent filmInformation provided by 3M
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ 1000-38 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ ElectroCut™ 7125-38 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ ElectroCut™ 7725-276 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ ElectroCut™ 7725-307 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ 1000-27 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ 1000-63 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | |
|
3M Scotchcal™ 3632-20 Translucent Film
2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | Type IV, 510 mm/min; ASTM D638 |
|
PolyOne Syncure™ S1054A Polyethylene, Crosslinked (XLPE)
Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Oven Aging, Tensile, Elongation, Deformation, Hot Creep, and Gel measured on a 95 phr S1054..
|
|||
| Tensile Strength at Break | 17.2 MPa | 2490 psi | 5mm/min; ASTM D638 |
|
Mitsui TPX® MX004 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
|
|||