| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 18.6 - 20.7 MPa | 2700 - 3000 psi | |
|
ITW Plexus Plexusâ„¢ AO420 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive , high toughness.Information provided by Illinois Tool Works.
|
|||
| Tensile Strength at Break | 17.2 - 20.7 MPa | 2500 - 3000 psi | |
|
ITW Plexus Plexusâ„¢ MA556 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Information provided by Illinois Tool Works..
|
|||
| Tensile Strength at Break | 17.2 - 20.7 MPa | 2500 - 3000 psi | |
|
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois ..
|
|||
| Tensile Strength at Break | 18.6 - 20.7 MPa | 2700 - 3000 psi | |
|
ITW Plexus Plexusâ„¢ MA920 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, short open time.Information provided by Illinois Tool Works.
|
|||
| Tensile Strength at Break | 17.2 - 20.7 MPa | 2500 - 3000 psi | |
|
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works.
|
|||
| Tensile Strength at Break | 13.8 - 20.7 MPa | 2000 - 3000 psi | |
|
Abatron AboCast 7802-1/AboCure 50-3 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, ..
|
|||
| Tensile Strength at Break | 13.8 - 20.7 MPa | 2000 - 3000 psi | |
|
Abatron AboCast 7802-1/AboCure 7804-4 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia..
|
|||