| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 65.5 MPa | 9500 psi | 2 in/min; ASTM D638 |
|
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | 2 in/min; ASTM D638 |
|
RheTech Products GC30P200-523 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, (GM 167A) Ebony
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | chs 2 in/min; ASTM D638 |
|
Network Polymers MS 100 Styrene Methyl Methacrylate Copolymer
Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc.
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Polymer Resources PC-HM-FR1-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | TM R050-36 |
|
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy
EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Polymer Resources PC-UV4 Polycarbonate, UV-stabilized, Easy Flow
Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Polymer Resources PC-UV4-[color]-1 Polycarbonate, UV-stabilized, Easy Flow with Mold Release
Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Ravago Manufacturing Americas Hylon® N1000EHL Nylon 6/6 (Cond)
(discontinued **)
Information provided by Ravago
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | 2.0 in/min; ASTM D638 |
|
LTL Color Compounds ColorFast® PC200 Polycarbonate
20 melt superior processing, fast cyclingAll information provided by LTL Color Compounders, Inc.
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | 50 mm/min; ASTM D638 |
|
Styron CALIBREâ„¢ 2061-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 2061-22 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-22 provides exceptional clarity, heat resistance, impa..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | 50 mm/min; ASTM D638 |
|
Styron CALIBREâ„¢ 200-23 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-23 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
|
|||
| Tensile Strength at Break | >= 65.5 MPa | >= 9500 psi | |
|
Master Bond Supreme 10HTCL Epoxy for Cryogenic Applications
Description: Master Bond Supreme 10HTCL features a blend of performance properties including both high shear and peel strengths along with convenient handling. This one component system is formulate..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Plastics Group Polifil® GFABS-10 10% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS)
Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire..
|
|||
| Tensile Strength at Break | >= 65.5 MPa | >= 9500 psi | |
|
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive
Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo..
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Entec Hylex® P1310FR Polycarbonate
Information provided by Ravago
|
|||
| Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
|
Entec Hylex® P1325L1 HB Polycarbonate