Polymer Property : Tensile Strength at Break = 6960 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 48.0 MPa
<= 6960 psi
ISO/R527
Polykemi AB POLYabs SN0 ABS
Information provided by Polykemi AB
Tensile Strength at Break <= 48.0 MPa
<= 6960 psi
ISO/R527
Polykemi AB POLYblend 45FS GKF2010 PC/ABS-Blend, Glass Fiber reinforced
Information provided by Polykemi AB
Tensile Strength at Break 48.0 MPa
6960 psi
50 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS
Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo..
Tensile Strength at Break 48.0 MPa
6960 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
Tensile Strength at Break 48.0 MPa
6960 psi
Type I, 50 mm/min; ASTM D 638
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Tensile Strength at Break 48.0 MPa
6960 psi
50 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® FXC810AL PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810AL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Alpine White colour effects. The colour package may effect performance.This data was..
Tensile Strength at Break 48.0 MPa
6960 psi
Type I, 50 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by ..
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D 638
SABIC Innovative Plastics LNP Colorcomp D10009 PC
LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied ..
Tensile Strength at Break 48.0 MPa
6960 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DI001L PC
LNP* LUBRICOMP* DI001L is a compound based on Polycarbonate resin containing 2% Silicone. Added characteristics of this grade are: Low Extractable.
Tensile Strength at Break 48.0 MPa
6960 psi
5 mm/min; ISO 527
SABIC Innovative Plastics Geloy FXTW30CP ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength at Break 48.0 MPa
6960 psi
5 mm/min; ISO 527
SABIC Innovative Plastics Lexan® HFD4271 PC (Asia Pacific)
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..
Tensile Strength at Break 48.0 MPa
6960 psi
ISO 527-1/-2
Lanxess Pocan® KU 2-7205 000000 PBT
PBT, non-reinforced, injection molding, extrusion, flame retardant
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D 638
SABIC Innovative Plastics LNP Lubricomp DP003F PC
LNP LUBRICOMP* DP003F is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the..
Tensile Strength at Break 48.0 MPa
6960 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KL002L Acetal
LNP* LUBRICOMP* KL002L is a compound based on Acetal Copolymer resin containing 10% PTFE. Added features of this grade include: Wear Resistant, Low Extractible.
Tensile Strength at Break 48.0 MPa
6960 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS
LNP* LUBRICOMP* ZP001XXP is a compound based on PPE+PS resin containing 5% PTFE/Silicone. Added features of this material include: Wear Resistant.
Tensile Strength at Break 48.0 MPa
6960 psi
Type I, 50 mm/min; ASTM D 638
SABIC Innovative Plastics Valox® 357U PBT
Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.This data was supplied by SABIC-IP for the Americas region.
Tensile Strength at Break 48.0 MPa
6960 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Tensile Strength at Break 48.0 MPa
6960 psi
50mm/min; ISO 527
Teijin Multilon TN-7500F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. High stiffness and flowability realize the thin wall of large-scale business machine chassis.Information provided by Tei..
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP WX05456 Polyester, TP
LNP THERMOCOMP* WX05456 is a compound based on Polyester, TP resin containing Mineral.
Tensile Strength at Break 48.0 MPa
6960 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA
NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate..
Tensile Strength at Break 48.0 MPa
6960 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PN275F PPE+PS
PPE+PS with low mineral loading. High heat, platable applications. NSF approved for water contact applications.
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D638
Toyobo VYLOPET® EMC605P PBT/PET Alloy, Anti-microbial
Applications: Gas equipment partsFeatures: Good anti-microbialGood appearanceFlame resistantInformation provided by Toyobo.
Tensile Strength at Break 48.0 MPa
6960 psi
ISO 527-2
Total PSC 1160/1160N Crystal Polystyrene
1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. Most notable for the production of bi-oriented polystyrene (BOPS). It is particularly useful..
Tensile Strength at Break 48.0 MPa
6960 psi
50mm/min; ISO 527-2
Denka MALECCA K-095 ABS
A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de..
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D412
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer
Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D638
Ravago Manufacturing Americas Echo® RPC10G BK Polypropylene Homopolymer
Available in North America Filler: Glass Fiber Reinforcement, 10% Filler by weight Recycled Content: YesFeatures: Homopolymer Color: Black Form: Pellets Information provided by Ravago.
Tensile Strength at Break 48.0 MPa
6960 psi
5 mm/min; ISO 527
SABIC Innovative Plastics Lexan® HFD4271 PC (Europe-Africa-Middle East)
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..
Tensile Strength at Break 48.0 MPa
6960 psi
50 mm/min; ISO 527
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific)
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
Tensile Strength at Break 48.0 MPa
6960 psi
50 mm/min; ISO 527
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
Tensile Strength at Break 48.0 MPa
6960 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics Xenoy® X6800BM PBT (Europe-Africa-Middle East)
Blow moldable, impact modifed XENOY