Mechanical Properties Metric English Comments
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105-7194/GY PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105-7460/BL5019 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Chemical and hydrolysis resistance parts, non flamm..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105-8135/GN PEEK, unreinforced, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105-8135/VI PEEK, unreinforced, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105-8279 PEEK, with CNT
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1301-7662/BK PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 50/CF/10/TF/15/BK 100 Polycarbonate, with carbon fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 50-7154 Polycarbonate, with carbon fiber, low-warpage
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 50-8076 Polycarbonate, with carbon fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 6-8159 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 80-7555 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 80-7713 Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 80-7713-NA Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOTECH® GS 46 Polyamide 46, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Highly dimensionally stable at e..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss ELECTRAFIL M-2386 Polycarbonate, with carbon fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105/BK0873 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Especially suitable for medical parts, super..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105/BK7308 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105/BK7308-1 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105/GN7348 PEEK, unreinforced, laser markable
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Not flammable.Especially suitable for medica..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105/GY7993 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105/WT106 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105-0831 PEEK, unreinforced, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105-7018/GN PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105-7106 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105-7685 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Super..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1700-1401 PPO, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1-0865 Polyamide 66, with aramid reinforcement, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1105-8135/OR PEEK, unreinforced, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Tensile Stress 100 MPa
14500 psi
Lehmann & Voss LUVOCOM® 1200-7116-2 ABS, with carbon fiber
Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff ..
Copyright © lookpolymers.com All Rights Reserved