Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVALEN PC 51 C 40 LS/1M Polypropylene reinforced with mineral filler, UV stabilized
Modified copolymer PP for injection molding with the content of 40% mineral filler, UV stabilized. Product meets glow wire test at 750°C. Delivered in full RAL color scale.Information Provided by P..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PC 51 C 40 PP reinforced with 40% mineral filler
Features: Modified homopolymer and copolymer PP for injection moulding with the contenct of 40% microground, chemically modified chalk. Increased strength, rigidity and thermal application up to 100..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PC 71 GF 10 PP, 10% glass fibre
FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass fibre and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVALEN PH 56 FRD 1 Polypropylene Homopolymer, Halogen Flame Retardant
FeaturesModified homopolymer PP for injection moulding with increased flammability resistance. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil form..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6 GF 10 FRC 2 PA6, 10% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically strengthened with 10 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVAMID 6 GF 15 LS Polyamide 6, 15% Glass Fiber, UV Stabilization
FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools...
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 5 T 20 FRG 2 PA6, 5% glass fibre, 20% mineral filling
FeaturesPA 6 for injection moulding, with halogen free flame retardant based on polyphosphate. Good anisotrophi shinking. Application for the electrical industry: protectors, coil forms, covers, ter..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVAMID 66 GF 10 GB 20 Polyamide 66, 10% Glass Fiber, 20% Glass Beads
FeaturesPA 66 chemically reinforced with 10% glass fiber and with the content of 20% glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can ..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -40.0 °C
9.52 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
LATI LARIL 13 G/20-V1 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -40.0 °C
9.52 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
LATI LARIL 13 G/20-V1 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
LATI LARIL 13 G/20-V1 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
LATI LATAN 13 G/303 30% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)  (discontinued **)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
LATI Latene® 7H2W T-V0E PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Low smoke density and low toxicity i..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant
Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 0.000 °C
9.52 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eU
Inno-Comp INNOPOL® CS 1-2120 AP 20% Talc Filled Polypropylene Homopolymer
INNOPOL CS 1-2120 AP is a 20 % talc filled compound based on polypropylene homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 1-2120 AP is recommended especially..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Pocan® B 3215 901510 PBT, 10% Glass Fiber
PBT, 10% glass fibers, injection molding
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem 2412EPR PEI
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 21 T 20 PP, 20% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® N2520 XL2 POM
Description: Is a POM, injection-molding grade with increased electrical conductivity, for applications with reduced mechanical requirements.Information provided by BASF
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion ..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion ..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 91 C 20 PP, 20% mineral filling
FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
LATI LARTON G/40 40% Glass Fiber Filled Polyphenylene sulfide (PPS)  (Unverified Data**)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -40.0 °C
9.52 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
LATI LARTON G/40 40% Glass Fiber Filled Polyphenylene sulfide (PPS)  (Unverified Data**)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXALEN PPH329B20 Polypropylene Homopolymer, 20% Glass Filled
SAXALEN PPH329B20 is a 20% glass beads filled Polypropylene - Homopolymer intended for injection molding. Low shrinkage, low warpage gradeInformation provided by SAX Polymers