| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
STN EN ISO 179 |
|
Plastcom SLOVALEN PC 51 C 30 Polypropylene Homopolymer and Copolymer, 30% Micronized Talc
FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 30% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C...
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -20.0 °C
|
21.4
ft-lb/in² <br>@Temperature -4.00 °F
|
|
|
Plastcom SLOVAMID 66 GB 30 GF 20 PA66, 20% glass fibre, 30% glass beads
FeaturesPA 66 chemically reinforced with 20% glass fibre and with the content of 30 % glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can b..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
|
|
Plastcom SLOVAMID 66 GF 14 HI TS PA66, 14% glass fibre, improved strength
FeaturesChemically reinforced with 14% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -20.0 °C
|
21.4
ft-lb/in² <br>@Temperature -4.00 °F
|
STN EN ISO 179 |
|
Plastcom SLOVAMID 66 GF 25 FRG 5 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 66 for injection moulding, chemical reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -20.0 °C
|
21.4
ft-lb/in² <br>@Temperature -4.00 °F
|
|
|
Plastcom SLOVAMID 66 GF 25 FRI 3 TS PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -20.0 °C
|
21.4
ft-lb/in² <br>@Temperature -4.00 °F
|
STN EN ISO 179 |
|
Plastcom SLOVASTER® B GF 20 Polybutylene Terephthalate, 20% Glass Fiber
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -20.0 °C
|
21.4
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179 |
|
Polykemi AB POLYfill PP CQX10030E10 F Polypropylene, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -20.0 °C
|
21.4
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179 |
|
Polykemi AB POLYfill PP CQX10030E10 Polypropylene, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
|
|
Radici Radilon® S RCV3015 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
DSM Akulon® K-FHGM35 (Cond.) 40% Glass/Mineral Reinforced, Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eU |
|
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179-1eU |
|
Lanxess Durethan® BKV 15 H.3 DUS008 000000 Nylon 6, 15% Glass Fiber
PA 6, 15% glass fibers, injection molding, heat-ageing stabilizedInformation provided by LANXESS.
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
Lanxess Durethan® BKV 20 FN00 000000 Nylon 6, 18% Glass Fiber
PA6, injection molding grade, 18% glass fibers, UL94 V-0 at 0,75 mm ( in house test), free of halogen and red phosphorus, specially for electro/electronic applications in regard to IEC60335-1
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eU |
|
Lanxess Pocan® B 3225 000000 PBT, 20% Glass Fiber
PBT, 20% glass fibers, injection molding
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1fU |
|
Styron INSPIREâ„¢ DLGF 9631.01 Z Polypropylene homopolymer, 60% LGF
Overview: DLGF 9631.01 Z is based on polypropylene homopolymer and reinforced with 60% by weight of long glass fiber. (PP-LGF 60, Long Glassfiber Granulate). DLGF 9631.01 Z is produced by pultrusion..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
DSM Akulon® K222-KGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eU |
|
DSM Akulon® K224-G3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
dry; ISO 179/1eU |
|
DSM Akulon® K224-PG2 PA6-I-GF8
8% Glass Reinforced, Impact Modified
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
DSM Arnite® TV4 461 (PBT+PET)-GF30
30% Glass Reinforced
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
dry; ISO 179/1eU |
|
DSM Novamid® 1010GN7-20 BK37 PA6-GF20 FR(30) 0
20% Glass Reinforced, Flame Retardant, Halogen free
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/eU |
|
Eurotec® Tecodur® PB70 GR30 NL CA 01 PBT/PET 30% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eU |
|
DSM Akulon® K224-G3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eU |
|
DSM Akulon® K224-HG3 (Dry) 15% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eU |
|
DSM Arnite® B436 SE PBT-GF30 FR(17)
30% Glass Reinforced, Flame Retardant
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/eU |
|
Eurotec® Tecodur® PB70 GR15 NL PBT 15% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
DSM Arnite® TV4 241 SL PBT-GF20 FR(17)
20% Glass Reinforced, Flame Retardant, UV Stabilized
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
|
|
Plastcom SLOVAMID 6 GB 20 PA6 reinforced with 20% glass beads
Features: Nearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical proper..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
STN EN ISO 179 |
|
Plastcom SLOVAMID 6 T 30 Polyamide 6, 30% Micronized Talc
FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
DSM Akulon® K220-HGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Cond)
(discontinu
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||