| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
|
Plastcom PLASTAMID® 6 GF 30 005 PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 30% glass fiber, used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
|
Plastcom SLOVAMID 6 GF 15 Polyamide 6, 15% Glass Fiber
FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and ..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
|
|
Plastcom SLOVAMID 6 GF 30 FRA 3 PA6, 30% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 850°C,..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
|
|
Plastcom SLOVAMID 66 GF 20 HI PA66, 20% glass beads
FeaturesChemically reinforced with 20% glass beeds, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Injection Molded; ISO 179 |
|
PolyOne Bergamid™ B70 G/GK30 TM-Y UV NC Polyamide 6 (Nylon 6)
Information provided by PolyOne
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
DSM Akulon® K224-G3U (Cond.) 15% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® B 31 F 000000 Nylon 6, Film Grade
PA 6, film grade, low viscosity, easy flow, additive-freeApplication Examples: flat and blown film, monofilaments, coatings
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
|
Lanxess Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant, improved flowabilityInformation provided by LANXESS.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Lanxess Pocan® DP BF 4232 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
|
|
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -20.0 °C |
26.2
ft-lb/in² @Temperature -4.00 °F |
|
|
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 179-1eU |
|
Lanxess Durethan® BKV 30 N1 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Valox® VX5005 PBT (Europe-Africa-Middle East)
VALOX VX5005 is a 5% glass fibre reinforced, impact modified PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Sax Polymers SAXAMID 226F5 Nylon 6.6, 25% Glass Fiber
SAXAMID 226F5 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has high mechanical strength in combination with good flow properties.Information provid..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1fU |
|
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/BJ356MO
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eU |
|
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30
30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
|
Eurostar Staramide AG6H PA66, 30% Glass Filled, Injection Molded
AG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
|
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded
AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
|
Eurotec® Tecodur® PB70 GR15 NL TD 28 PBT 15% glass fiber reinforced, UL94 V0, impact modified, high CTI
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
|
Eurotec® Tecodur® PB70 GR50 NL PBT 50% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
|
Eurotec® Tecomid® NB40 NL XA 20 PA 6 unreinforced, UL94 V0
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
|
Eurotec® Tecodur® PB70 GR20 NL PBT 20% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
|
Eurotec® Tecomid® NA40 GR20 NL PA 6.6 20% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
|
|
Radici Radiflam® A RV300AE (cond.) Nylon 66-30GF
PA66 flame retardant injection molding grade. 30% Glass fiber reinforced, for items with high stiffness. Natural colorInformation provided by Radici group.
|
|||