Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 28.6 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -20.0 °C
28.6 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom PLASTAMID® 6 BT SD PA6
Basic type PA 6 for compounding, modified for general use. Grade can contain PA 66 up to 5% and TiO2 content up to 0.25 %. Use: automotive, engineering, electrical and consumer-goods industryInforma..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PC 81 T 30 PP, 30% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -20.0 °C
28.6 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVAMID 6 GF 30 FRG 5 Polyamide 6, 30% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -20.0 °C
28.6 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVAMID 66 W 40 Polyamide 66, 40% Mineral Filled
FeaturesPA 66 with the content of 40% chemically modified mineral filler. Used for grips of electric hand tools, hobby tools, gear wheels, covers of electric tools, flat products, automobile wheel ..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
PolyOne Bergamid™ A70 G25 H natur TM-X Polyamide 66 (Nylon 66)
Information provided by PolyOne
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DSM Akulon® K224-G3U (Dry) 15% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, suitable for GIT (gas assisted technology), good surface finish, good heat-ageing resistance
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Durethan® AKV 30 H2.0 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding-grade, 30% glass fibers, good heat-ageing resistance
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
d.a.m.; ISO 179-1eU
Lanxess Durethan® AM 40 X H2.0 901510 Nylon 66, Glass Fiber/Mineral Reinforced
PA 66, 40% glass fibers/mineral, injection molding, heat-aging stabilized, low tendency to warpInformation provided by LANXESS.
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
d.a.m.; ISO 179-1eU
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Lanxess Pocan® B 4239 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Pocan® B 3235 901510 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXATEC 6120 AES
SAXATEC 6120 is a easy lowing, weatherable AES injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX Polym..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polyram PlusTek PA840G13 Nylon 66 for Injection Molding, 13% Glass Fiber Reinforced, Impact Modified, Heat Resistant
Impact modified, 13% glass fiber reinforced, heat resistant Nylon 66 for injection molding applications.Information provided by Polyram.
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DSM Akulon® K224-G4U (Dry) 23% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DSM Arnite® TV4 261 PBT-30% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
Edgew 80x10x4 sp=62; ISO 179/1eU
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded
AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eU
Eurotec® Tecomid® NA40 GR25 NL XA 42 PA 6.6 25% glass fiber reinforced, UL94 V0, red phosphorus
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eU
Eurotec® Tecomid® NA40 GR25 NL PA 6.6 25% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179-1eU
Barlog Plastics KEBATER BF130 PBT, 30% glass fiber reinforced
PBT-GF30Information provided by BARLOG plastics GmbH.
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Akro-Plastic Akromid® T1 GF 40 (3464) PPA Dry, 40% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PC 91 T 30 PP, 30% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif..
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East)
VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load..
Copyright © lookpolymers.com All Rights Reserved