Mechanical Properties Metric English Comments
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
STN EN ISO 179
Plastcom PLASTAMID® 66 BT B 27 A/IM PA66
Basic type PA66 for injection molding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fas..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -20.0 °C
38.1 ft-lb/in²
<br>@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVAMID 6 GF 45 Polyamide 6, 45% Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
Plastcom SLOVAMID 66 GF 25 FRA 5 PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, reinforced with 25% glass fibre and halogen flame retardant. Application in electrical industry: breakers, coilforms, covers, terminals. Slightly decreased flam..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -20.0 °C
38.1 ft-lb/in²
<br>@Temperature -4.00 °F
Plastcom SLOVAMID 66 GF 25 FRA 5 PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, reinforced with 25% glass fibre and halogen flame retardant. Application in electrical industry: breakers, coilforms, covers, terminals. Slightly decreased flam..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
Plastcom SLOVAMID 66 GF 35 HTS PA66, 355% glass fibre, combined stability
FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fibre, heat stabilized and stabilized against hydrolysis. Used for cooling water systems in the automotive industry. Delive..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -20.0 °C
38.1 ft-lb/in²
<br>@Temperature -4.00 °F
Plastcom SLOVAMID 66 GF 45 PA66, 45% glass fibre
FeaturesChemically reinforced with 45% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
Radici Radilon® A CP400 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
Radici Radilon® A RV300 990 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
d.a.m.; ISO 179-1eU
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS.
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -30.0 °C
38.1 ft-lb/in²
<br>@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Lanxess Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30 H3.0, ev..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -30.0 °C
38.1 ft-lb/in²
<br>@Temperature -22.0 °F
cond.; ISO 179-1eU
Lanxess Durethan® BKV 140 H2.0 DUS008 900051 Nylon 6, Glass Fiber Reinforced, Impact Modified
PA 6, 40% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -30.0 °C
38.1 ft-lb/in²
<br>@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Lanxess Durethan® BKV 215 H2.0 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning ..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -30.0 °C
38.1 ft-lb/in²
<br>@Temperature -22.0 °F
d.a.m.; ISO 179-1eU
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced
PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS.
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -20.0 °C
38.1 ft-lb/in²
<br>@Temperature -4.00 °F
LATI Latamid 66 E21 G/15 PA 66, 15% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -30.0 °C
38.1 ft-lb/in²
<br>@Temperature -22.0 °F
cond.; ISO 179-1eU
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant
PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS.
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
Lanxess Durethan® BKV 30 HTS 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, very good heat-ageing resistance
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
conditioned; ISO 179-1eU
Lanxess Durethan® BKY 115 H3.0 DUS008 Nylon 6, 15% Glass Fiber
PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS.
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -30.0 °C
38.1 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
Lanxess Pocan® B 2505 000000 PBT
PBT, non-reinforced, injection molding, flame retardant
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -30.0 °C
38.1 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS
Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -30.0 °C
38.1 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXAMID 126F6 Nylon 6, 30% Glass Fiber
SAXAMID 126F6 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Other properties are ..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -30.0 °C
38.1 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXAMID 126F7 Nylon 6, 35% Glass Fiber
SAXAMID 126F7 is a polyamide 6 injection-molding-grade reinforced with 35% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Additional properties..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Borealis HF700SA Polypropylene
HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
cond; ISO 179/1eU
DSM EcoPaXX® Q-KG6 PA410-GF30
% Glass Reinforced, Heat Stabilized, for E&E applications
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -30.0 °C
38.1 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -30.0 °C
38.1 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® N2720 M210 POM
Description: Is a POM, product with increased stiffness and strength as well as good wear characteristics, used, for instance, for sliding chains and conveyor systems.Information provided by BASF
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature -30.0 °C
38.1 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry)
Information provided by BASF
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
Lanxess Durethan® BKV 35 H2.0 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: automotive structures
Charpy Impact Unnotched 8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry)
Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el..