Polymer Property : Charpy Impact Unnotched = 5.00 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
STN EN ISO 179
Plastcom PLASTALEN® PH 91 SDU Polypropylene
Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in full RAL color.Information Provided by Plastcom spol. s r.o.
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -20.0 °C
23.8 ft-lb/in²
<br>@Temperature -4.00 °F
STN EN ISO 179
Plastcom PLASTAMID® 6 BT N 26 B/IM PA6
Basic type PA 6 for injection molding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools. Delivered in the natu..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -20.0 °C
23.8 ft-lb/in²
<br>@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVAMID 66 GF 25 Polyamide 66, 25% Glass Fiber
FeaturesChemically reinforced with 25% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVASTER® B1 GF 15 FRL 4 PBT reinforced with glass fibers, flame retarded
PBT reinforced with 15 % glass fiber, flame retarded with the halogen flame retardant. Anisotropy of shrinkage enables the injection molding of round, cylindrical or other hole products. Application..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -30.0 °C
23.8 ft-lb/in²
<br>@Temperature -22.0 °F
Radici Radiflam® A RV250AF (dry) Nylon 66-25GF
Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/2C
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East)
LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
DSM Arnite® TV4 460 KL TV4 460 PBT/PET Blend-30% Glass Reinforced (European Grade) &nbsp;(discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -20.0 °C
23.8 ft-lb/in²
<br>@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVASTER® B GF 30 FRL 4 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant
FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -30.0 °C
23.8 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
DSM Arnite® AV2 370 /B AV2 370 PET-35% Glass Reinforced (European and Asian Grade) &nbsp;(discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
DSM Akulon® Ultraflow™ K-FHGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Cond) &nbsp;(d
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -30.0 °C
23.8 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow)
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -30.0 °C
23.8 ft-lb/in²
<br>@Temperature -22.0 °F
d.a.m.; ISO 179-1eU
Lanxess Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX152R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -30.0 °C
23.8 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
DSM Akulon® S223-HPG5 Impact Modified Nylon 66-25% Glass Reinforced (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -30.0 °C
23.8 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
DSM Akulon® S223-HPG5 Impact Modified Nylon 66-25% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -30.0 °C
23.8 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
DSM Arnite® TV4 260 SN PBT-GF30 FR(17)
30% Glass Reinforced, Flame Retardant
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -30.0 °C
23.8 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
DSM Arnite® TV6 240 PBT-GF20
20% Glass Reinforced
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -30.0 °C
23.8 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
DSM Akulon® K224-HG3 (Dry) 15% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -30.0 °C
23.8 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
DSM Arnite® TV6 241 SN PBT-GF20 FR(17)
20% Glass Reinforced, Flame Retardant
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVASTER® B GF 20 FRL 4 Polybutylene Terephthalate, 20% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant
FeaturesPBT with the content of 20% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXALEN PPC339T20 Polypropylene Copolymer, 20% Talc Filled
SAXALEN PPC339T20 is a 20% mineral filled Polypropylene - Copolymer intended for injection molding with good flow properties und higher stiffness. The PP-Copolymer has low warpage behaviors and good..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -20.0 °C
23.8 ft-lb/in²
<br>@Temperature -4.00 °F
LATI Latamid 66 H2 G/25-V0KB3 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature -30.0 °C
23.8 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
DSM Arnite® TV4 260 SF PBT-30% Glass Reinforced (European and Asian Grade) &nbsp;(discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
Lanxess Pocan® TP 740-201 000000 PBT + ASA, 20% Glass Fiber &nbsp;(discontinued **)
PBT+ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finish
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179-1eU
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber
PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
conditioned; ISO 179-1eU
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber
PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS.