| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
|
Plastcom SLOVAMID 6 GF 15 Polyamide 6, 15% Glass Fiber
FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and ..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
|
|
Plastcom SLOVAMID 6 GF 20 FRG 3 PA6, 20% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 20 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 9..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
|
Plastcom SLOVAMID® 6 GF 20 FRA 5 PA6 reinforced with glass fiber, flame retarded
PA 6 for injection molding, reinforced with 20% glass fiber, flame retarded with halogen flame retardant. Main features: flammability in accordance with UL 94 5 at 1.6 mm, glow wire at 960°C. Appli..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -20.0 °C |
26.2
ft-lb/in² @Temperature -4.00 °F |
|
|
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
|
Plastcom SLOVALEN PH 49 GF 30 003/3M Polypropylene reinforced with glass fiber, heat stabilized
Modified homopolymer PP for injection molding, reinforced with 30% glass fiber, heat stabilized. Delivered in black color.Information Provided by Plastcom spol. s r.o.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
|
|
Plastcom SLOVAMID 6 GF 15 MI/2 PA6, 15% glass fibre, improved strength
FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
DSM Akulon® K224-G3U (Cond.) 15% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Lanxess Durethan® BKV 35 H2.0 EF 900116 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow)
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® BKV 35 H2.0 EF 900116 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow)
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® BKV 35 HTS 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, very good heat-ageing resistance
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eU |
|
Lanxess Pocan® ECO T 3230 000000 PBT + PET, 30% Glass Fiber
PBT + PET, 30% glass fibers, injection molding, improved surface finish, contains 30% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® BKV 30 H2.0 EF 900116 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66
NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Sax Polymers SAXAMID 226F5 Nylon 6.6, 25% Glass Fiber
SAXAMID 226F5 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has high mechanical strength in combination with good flow properties.Information provid..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/HK060AE
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
DSM Akulon® K225-KS (Dry) Flame Retardant (Halogen free), Heat Stabilized Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eU |
|
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30
30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
|
Eurostar Staramide RF006SXP PA66, 30% Glass Fiber Filled, Injection Molded
Staramide RF006SXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
|
Eurostar Staramide RF006SXS PA66, 30% Glass Fiber Filled, Injection Molded
Staramide RF006SXS is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4; ISO 179/1eU |
|
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded
AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
|
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded
BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
|
Barlog Plastics KEBATER BF250 PBT, 50% glass fiber reinforced, food grade
PBT-GF50Information provided by BARLOG plastics GmbH.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher ..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
|
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded
BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
|
|
Radici Radilon® A RV300 990 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -40.0 °C |
26.2
ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eU |
|
Polyplastic Armlen® PP GF 30-1EX Polypropylene Copolymer, 30% Glass Fiber
Information provided by PolyPlastic Group.
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature -30.0 °C |
26.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Lanxess Pocan® A 3131 000000 PBT+ASA, 30% glass fibers
PBT+ASA, 30% glass fibers, injection molding, low tendency to warp, improved surface finish
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
Sax Polymers SAXALEN PPH327G28 Polypropylene Homopolymer, 28% Glass Filled
SAXALEN PPH327G28 is a 28% glass filled Polypropylene - Homopolymer injection molding grade with increased stiffness.Information provided by SAX Polymers
|
|||
| Charpy Impact Unnotched |
5.50
J/cm² @Temperature 23.0 °C |
26.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
|
LG Chemical HG-174 ABS, High Gloss, Super High Flow
Information Provided by LG Chem
|
|||