| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
|
Plastcom SLOVAMID 6 GF 30 LS Polyamide 6, 30% Glass Fiber, UV Stabilization
FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools...
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
|
|
Plastcom SLOVASTER® B1 GF 20 000/2 PBT, 20% glass fibre
FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre, excellent flow. Characterised by excellent properties also at minus temperatures like eg. modu..
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
PolyOne Bergamid™ A700 G25 U-SO Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
|
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**)
Zytel® 70G25HSLR NC010 is a 25% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
|
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**)
Zytel® 70G25HSLR NC010 is a 25% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
DSM Akulon® K224-HG5 (Cond.) 25% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued *
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
|
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**)
Minlon® 73GM40 NC010 is a 40% mineral/glass reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
|
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**)
Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, suitable for GIT (gas assisted technology), good surface finish, good heat-ageing resistance
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179-1eU |
|
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers
PA 66, 30% glass fibers, injection molding, heat-ageing stabilized
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® BCF 30 X H2.0 901510 Nylon 6, 30% Glass + Carbon Fiber
PA 6, injection molding grade, 30% reinforced (glass fibers + carbon fibers), conductive, intrinsic color black, good heat-ageing resistance
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber
PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
Lanxess Pocan® B 3225 XF 000000 PBT, 20% Glass Fiber
PBT, 20% glass fibers, injection molding, improved flowability
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
|
Lanxess Pocan® ECO T 3240 000000 PBT + PET, 45% Glass Fiber
PBT + PET, 45% glass fibers, injection molding, improved surface finish, contains 25% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS.
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Lanxess Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
|
Lanxess Durethan® BKV 30 N1 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Akulon® K225-KS (Dry) Flame Retardant (Halogen free), Heat Stabilized Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eU |
|
DSM EcoPaXX® Q-KG6 PA410-GF30
% Glass Reinforced, Heat Stabilized, for E&E applications
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
|
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded
AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Arnite® AV2 370 HF PET-GF35
35% Glass Reinforced, Brake Booster Body Valves, High Flow
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
|
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Arnite® TV6 260 T PBT-I-GF30
30% Glass Reinforced, Improved Impact
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
DSM Akulon® K-FKGS6 (Dry) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature 23.0 °C |
28.6
ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif..
|
|||
| Charpy Impact Unnotched |
6.00
J/cm² @Temperature -30.0 °C |
28.6
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Lanxess Pocan® DP B 3235 XF 901510 PBT, 30% Glass Fiber
(discontinued **)
PBT, 30% glass fibers, injection molding, improved flowability
|
|||