| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
STN EN ISO 179 |
|
Plastcom PLASTAMID® 66 BT N 27 B PA66
PA66 for compounding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, h..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
STN EN ISO 179 |
|
Plastcom PLASTAMID® 66 BT N 27 B/IM PA66
PA66 for injection molding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, cla..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature -20.0 °C
|
35.7
ft-lb/in² <br>@Temperature -4.00 °F
|
|
|
Plastcom SLOVAMID 66 GF 20 GB 10 HI PA66, improved strength
FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
|
|
Plastcom SLOVAMID 66 GF 25 FRI 2 PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
STN EN ISO 179 |
|
Plastcom SLOVAMID 66 GF 35 FRG 5 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 66 for injection moulding, chemical reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
STN EN ISO 179 |
|
Plastcom SLOVAMID 66 GF 35 Polyamide 66, 35% Glass Fiber
FeaturesChemically reinforced with 35% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
|
|
Radici Radilon® A RV150 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
DAM; ISO 179/1eU |
|
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**)
Zytel® 70G30HSL BK039B is a 30% glass reinforced, heat stabilized, black nylon 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature -30.0 °C
|
35.7
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eU |
|
DSM Akulon® K224-TG9/A Nylon 6-45% Glass Reinforced (European Grade) (Cond)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
Lanxess Durethan® AKV 30 H2.0 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding-grade, 30% glass fibers, good heat-ageing resistance
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature -30.0 °C
|
35.7
ft-lb/in² <br>@Temperature -22.0 °F
|
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
Conditioned; ISO 179-1eU |
|
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres
PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature -30.0 °C
|
35.7
ft-lb/in² <br>@Temperature -22.0 °F
|
cond.; ISO 179-1eU |
|
Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
Lanxess Durethan® BKV 35 HTS 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, very good heat-ageing resistance
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
Lanxess Durethan® DP AKV 30 X HR EF 900116 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, hydrolysis and good heat-ageing resistance, good flowability (Easy Flow)
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
Lanxess Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature -20.0 °C
|
35.7
ft-lb/in² <br>@Temperature -4.00 °F
|
|
|
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature -30.0 °C
|
35.7
ft-lb/in² <br>@Temperature -22.0 °F
|
dry; ISO 179/1eU |
|
DSM Stanyl® TE200F8 PA46-GF40
40% Glass Reinforced, Heat Stabilized, for E&E applications
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
Edgew 80x10x4 sp=62; ISO 179/1eU |
|
Eurostar Staramide RF006SXS PA66, 30% Glass Fiber Filled, Injection Molded
Staramide RF006SXS is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar.
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature -30.0 °C
|
35.7
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/eU |
|
Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM
Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature -30.0 °C
|
35.7
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eU |
|
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry)
Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
Polyplastic Armamid® PA6 GF 30-2HSM-902 Nylon, 30% Glass Filled
Heat stabilizedInformation provided by PolyPlastic Group.
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature -30.0 °C
|
35.7
ft-lb/in² <br>@Temperature -22.0 °F
|
|
|
Radici Radilon® A RV300R (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM
Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin..
|
|||
| Charpy Impact Unnotched |
7.50
J/cm² <br>@Temperature 23.0 °C
|
35.7
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph..
|
|||