| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -20.0 °C |
71.4
ft-lb/in² @Temperature -4.00 °F |
|
|
Plastcom SLOVASTER® B1 BT PBT, basic type
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -20.0 °C |
71.4
ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
|
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)
(Unverified Data**)
Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper..
|
|||
| Charpy Impact Unnotched |
>=
15.0
J/cm² @Temperature 23.0 °C |
>=
71.4
ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
|
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -30.0 °C |
71.4
ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® A 30 S 000000 Nylon 66
PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature 23.0 °C |
71.4
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
Lanxess Durethan® A 30 S 000000 Nylon 66
PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature 23.0 °C |
71.4
ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 179-1eU |
|
Lanxess Durethan® A 30 S H3.0 000000 Nylon 66, Injection Molding
PA 66, non-reinforced, injection moldingInformation provided by LANXESS.
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature 23.0 °C |
71.4
ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 179-1eU |
|
Lanxess Durethan® B 30 S F30 000000 Nylon 6, Flame Retardant
PA 6, non-reinforced, injection molding, flame retardantInformation provided by LANXESS.
|
|||
| Charpy Impact Unnotched |
>=
15.0
J/cm² @Temperature 23.0 °C |
>=
71.4
ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls
PA6, molding grade, micro glass balls, good heat-ageing resistance
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -30.0 °C |
71.4
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Lanxess Pocan® B 1300 000000 PBT
PBT, non-reinforced, injection molding, extrusion
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -30.0 °C |
71.4
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Lanxess Pocan® B 1305 000000 PBT
PBT, non-reinforced, injection molding
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -30.0 °C |
71.4
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Lanxess Pocan® KU 1-7301 000000 PBT
PBT, non-reinforced, injection molding, food contact
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature 23.0 °C |
71.4
ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
|
Ineos ABS Lustran® ABS E211 LNS013 Pellets (a-methylstyrene-SAN-modified), Extrusion Grade
Lustran® ABS E211 LNS013 is extrusion grade with high heat resistance. It is used for the production of molded plastic articles.
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -30.0 °C |
71.4
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Styrolution Luran® S 776 S Colored ASA
Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j..
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -30.0 °C |
71.4
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Styrolution Luran® S 776 S UV ASA
Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j..
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -30.0 °C |
71.4
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Styrolution Luran® S 796 M Colored ASA
Description: High-impact injection molding gr4ade with good flowability.Applications: Trim panels for goods vehicles.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature 23.0 °C |
71.4
ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
|
Styrolution Novodur® E211 ABS
Novodur E211 is a high heat extrusion grade and suitable for blow moldingInformation provided by Styrolution
|
|||
| Charpy Impact Unnotched |
<=
15.0
J/cm² @Temperature 23.0 °C |
<=
71.4
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
Styrolution Polystyrol 454 C GR 2 PS
Description: Polystyrol 454 C is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Applications: TV-front panels and back covers, VCR fronts..
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature 23.0 °C |
71.4
ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 179/1eU |
|
SYNTHOS Krasten® 662E High Impact Polystyrene
High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of demanding visual appearance plates, technical parts, sheets and molded pa..
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature 23.0 °C |
71.4
ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
|
Styrolution Terblend® N 3154 ASA / PA, 8% Mineral filled
Terblend N 3154 is an 8% mineral filled ABS/PA blend with good dimensional stability and enhanced rigidity.High dimensional stabilityEnhanced rigidityMineral filled (8%)Information provided by Styro..
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature 23.0 °C |
71.4
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
Borealis Daplen™ EG103AI Polypropylene Compound, Mineral Filled
Daplen™ EG103AI is a 15 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and high melt flow rate..
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -30.0 °C |
71.4
ft-lb/in² @Temperature -22.0 °F |
longitudinal; ISO 179/1eU |
|
Bond Laminates TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate
Within the TEPEX® composite laminate, Polyamide 66 is a resin known for its high hardness, stiffness, abrasion resistance, heat and chemical resistances. The carbon used within this material is ae..
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -30.0 °C |
71.4
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
BASF Ultraform® N2770 K POM
Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature 23.0 °C |
71.4
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
BASF Ultraform® N2770 K POM
Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -30.0 °C |
71.4
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
BASF Ultraform® W2320 003 PRO POM
Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature 23.0 °C |
71.4
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
BASF Ultraform® W2320 003 PRO POM
Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -30.0 °C |
71.4
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
BASF Ultraform® W2320 U03 POM
Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature -30.0 °C |
71.4
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by..
|
|||
| Charpy Impact Unnotched |
15.0
J/cm² @Temperature 23.0 °C |
71.4
ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
|
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.
|
|||