| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
|
|
Plastcom SLOVAMID 6 GF 50 TS PA6, 50% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature -20.0 °C |
45.2
ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
|
Plastcom SLOVAMID® 6 GF 65/2M PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 65% of glass fiber, for moldings used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby to..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
|
|
Radici Radilon® S RV300LK (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
|
|
Radici Radilon® S RV300R (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
|
|
Plastcom SLOVAMID 6 GF 50 LTS PA6, 50% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Akulon® S223-G8U (Dry) 43% Glass Reinforced Nylon 66 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
|
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**)
Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
|
Lanxess Durethan® BKV 130 H3.0 DUS008 000000 Nylon 6, 30% Glass Fiber
PA 6, glass fiber, injection molding, impact modified, heat-aged stabilizedInformation provided by LANXESS.
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eU |
|
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified
PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature -30.0 °C |
45.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eU |
|
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers
PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber
30% Glass fiber reinforced; injection molding grade
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
|
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature -30.0 °C |
45.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Sax Polymers SAXAMID 226F10 Nylon 6.6, 50% Glass Fiber
SAXAMID 226F10 is a polyamide 6.6 injection-molding-grade reinforced with 50% glass fibers. It has high mechanical strength.Information provided by SAX Polymers
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Akulon® K224-G6U (Dry) 33% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
|
DSM Akulon® K224-G8 PA6-GF40
40% Glass Reinforced
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Akulon® K224-HG6 (Dry) 30% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Akulon® K224-HG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Akulon® S223-HG7 (Dry) 35% Glass Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Akulon® S223-HPG5 Impact Modified Nylon 66-25% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Akulon® K224-G6 (Dry) 30% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
|
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, Conditioned
Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
|
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, Conditioned
Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature -30.0 °C |
45.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, Conditioned
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry)
Information provided by BASF
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
|
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Dry)
Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Akulon® K-FG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
DSM Akulon® K-FHG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature 23.0 °C |
45.2
ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
|
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
(Unverified Data**)
Zytel® RS 30G30L NC010 is a lubricated, 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer only). It was initia..
|
|||
| Charpy Impact Unnotched |
9.50
J/cm² @Temperature -30.0 °C |
45.2
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
DSM Akulon® K224-PG6 Impact Modified Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond)