Polymer Property : Izod Impact, Unnotched (ISO) = 21.4 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 45.0 - 50.0 kJ/m²

@Temperature -30.0 - -30.0 °C
21.4 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 47.5 kJ/m² Grade Count:2
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Izod Impact, Unnotched (ISO) 45.0 - 60.0 kJ/m²

@Temperature -30.0 - -30.0 °C
21.4 - 28.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 53.8 kJ/m² Grade Count:2
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL V01550 PPE+HIPS (Europe-Africa-Middle East)
NORYL V01550 is a 15 % short glass fibre reinforced, flame retardant material with a HDT/A of 130C according ISO 75. NORYL V01550 is V0 at 0.75 mm according UL94 and is halogen free according VDE/DI..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KA000 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Lubricomp* KA000 is a compound based on Acetal Copolymer resin containing Aramid Fiber, Proprietary Lubricant.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Asia Pacific)
LNP Lubricomp* KL004 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* Fu..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer (Asia Pacific)
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East)
VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 420HP PBT
30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180
Solvay Specialty Polymers Ryton® XE5515BL Polyphenylene Sulfide Alloy (PPS Alloy), 15% Glass Fiber
Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusi..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East)
VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East)
VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP LF006EL PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LF006EL is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding. FDA Compliant Raw Materials.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp M10009A PP (Europe-Africa-Middle East)
LNP* STARFLAM* M10009A is a compound based on Polypropylene resin, containing Flame Retardant. Added features include : Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middl..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Asia Pacific)
LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP UC008H PPA (Asia Pacific)
LNP* THERMOCOMP* UC008H is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP UF00ASW PPA
LNP* Thermocomp* UF00ASW is a compound based on Polyphthalamide (PPA) containing glass fiber. Characteristics of this grade of Heat Stabilized and Hot Water Moldable.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® HX420HP PBT
Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP DF008 PC
LNP THERMOCOMP* DF008 is a compound based on Polycarbonate resin containing 40% Glass Fiber.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp GX05053 PSU (Europe-Africa-Middle East)
LNP* THERMOCOMP* GX05053 is a compound based on Polysulfone blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ASTM D256
Tipco Tipcolite® VASW 200 Phenolic Compound, Long Glass Fiber, in fluffy form, Medium -Soft Flow & Very High Strength
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 180/1U
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starflam M10009A PP, Flame Retardant, Injection Molding
Starflam M10009A is an Unfilled Flame Retardant Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starflam PW0042E PA6, 20% Mineral Filled, Injection Molded
PW0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Reinforced, Polyamide 6 Injection MoldingInformation provided by Polymer Technology & Services, the North American exclus..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Staramide RF006K PA66, Glass Fiber Filled, Injection Molded
Staramide RF006K is a Radiation Crosslinkable, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ASTM D256
Beijing Ranger Chem PBT-201-G15 291 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ASTM D256
BLUESTAR 203G30 PBT, 30% Glass Filled
Typical Applications: Thinner wall partsInformation provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOTUF VX99810 Super Tough Nylon
Super Tough Nylon, Proprietary Filler(s),
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP JF002R PES (Europe-Africa-Middle East)
LNP* Thermocomp* JF002R is a compound based on Polyethersulfone resin containing Glass Fiber, Glass Bead. Added features of this material include: Mold Release.