Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched (ISO) = 21.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 46.0 kJ/m²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1eA
Mytex Polymers AS172LW-01US Thermoplastic Polyolefin, Compounded
AS172LW-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural, g..
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Cycoloy® C7240P PC+ABS (Asia Pacific)
Cycoloy* C7240P resin is a mineral filled, flame retardant PC/ABS. High stiffness combined with balanced flow and impact performance, makes it a good condidate for various applications.
Izod Impact, Unnotched (ISO) 46.0 - 48.0 kJ/m²
21.9 - 22.8 ft-lb/in²
Average value: 46.7 kJ/m² Grade Count:3
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Izod Impact, Unnotched (ISO) 46.0 kJ/m²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1eA
Mytex Polymers AS319LW-01US Thermoplastic Polyolefin, 19% Talc Filled
AS319LW-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural, g..
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Asia Pacific)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI
LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly
LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As..
Izod Impact, Unnotched (ISO) 46.0 kJ/m²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp RCP36XXP PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RCP36XXP is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Easy Molding, Internally Lu..
Izod Impact, Unnotched (ISO) 46.0 kJ/m²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp RCP36XXQ PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RCP36XXQ is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Easy Molding, Internally Lu..
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RFG16S PA 66
LNP* LUBRICOMP* RFG16S is a compound based on Nylon 66 resin containing 5% Graphite, 30% Glass Fiber. Added features of this material include: Heat Stabilized, Wear Resistant.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66
LNP LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% Lubricants. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA
LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT
LNP LUBRICOMP* WFP36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT (Asia Pacific)
LNP LUBRICOMP* WFP36 is a compound based on Polybutylene Terephalate resin containing Silicone, Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRILOY RF203AXH PA 66
LNP* LUBRILOY* RF203AXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP DF0089 PC
LNP THERMOCOMP* DF0089 is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Flame Retardant.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
GB/T 1843-2008
Sichuan Deyang Haton® hGR40DL Polyphenylene Sulfide, Glass Fiber Reinforced
Injection molding, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
GB/T 1843-2008
Sichuan Deyang Haton® hGR50 Polyphenylene Sulfide, Glass Fiber Reinforced
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RF006EXZ PA 66
LNP THERMOCOMP* RF006EXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²

@Temperature -30.0 °C
21.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East)
PPX630 is a 30% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. Generic identification acc. ISO11469: PP+PP..
Izod Impact, Unnotched (ISO) 46.0 kJ/m²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp XL004 Amorphous Polyamide
LNP* Lubricomp* XL-4040 is a compound based on Amorphous Nylon, containing PTFE.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66
LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66
LNP THERMOCOMP* RF006ESZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific)
LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOTUF WF003I Polyester, TP
LNP THERMOTUF* WF003I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled  (discontinued **)
LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat..
Copyright © lookpolymers.com All Rights Reserved