| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP KONDUIT ITF2B PA 6/12 (Asia Pacific)
LNP* Konduit* ITF2B is a compound based on Nylon 6/12 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180 |
|
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**)
AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re..
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica..
|
|||
| Izod Impact, Unnotched (ISO) |
28.0
-
90.0
kJ/m² @Temperature -30.0 - -30.0 °C |
13.3
-
42.8
ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 52.3 kJ/m² Grade Count:6 |
|
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific)
PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications.
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing 20% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Easy Molding, Electrically Conductive, Wear ..
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Easy Molding.
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP ZFG26 PPE+PS (Asia Pacific)
LNP* Lubricomp* ZFG26 is a compound based on PPE+PS Blend resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated.
|
|||
| Izod Impact, Unnotched (ISO) |
28.0
kJ/m² @Temperature -30.0 °C |
13.3
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East)
VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors.
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP STAT-KON DX05474 PC
LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold ..
|
|||
| Izod Impact, Unnotched (ISO) |
28.0
kJ/m² @Temperature 0.000 °C, Time 86400 sec |
13.3
ft-lb/in² @Temperature 32.0 °F, Time 24.0 hour |
|
|
Shandong Rike Chemical HELIâ„¢ HL-769 Weather-resistance Acrylic Impact Modifier (AIM)
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c..
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP STAT-KON EX99689C PEI
LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features include: Electrically Conductive, Easy Molding, Mold Release.
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific)
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release.
|
|||
| Izod Impact, Unnotched (ISO) |
28.0
kJ/m² @Temperature 23.0 °C |
13.3
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP Thermocomp EC002E PEI (Asia Pacific)
LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac..
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP JF004LZ PES
LNP* Thermocomp* JF004LZ is a compound based on PES containing 20% Glass Fiber. Added features include: Extrusion Grade, Low Extractible.
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific)
LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
|
|||
| Izod Impact, Unnotched (ISO) |
28.0
kJ/m² @Temperature 23.0 °C |
13.3
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP Lubricomp KFI12A Acetal Homopolymer
LNP LUBRICOMP* KFI12A is a compound based on Acetal Homopolymer resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABI..
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP STAT-KON DE0049P PC
LNP* STAT-KON* DE0049P is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. Electrically Conduct..
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched
LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP
LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized.
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT
LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific)
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180/1eU |
|
Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, DRY
Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.Available in: Asia Pacific, Europe, Latin America and North America..
|
|||
| Izod Impact, Unnotched (ISO) |
28.0
kJ/m² @Temperature -30.0 °C |
13.3
ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1U |
|
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific)
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated.
|
|||
| Izod Impact, Unnotched (ISO) |
28.0
kJ/m² @Temperature 23.0 °C |
13.3
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP Thermocomp MF0069S PP
LNP* Thermocomp* MF0069S is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant, Heat Stabi..
|
|||
| Izod Impact, Unnotched (ISO) | 28.0 - 55.0 kJ/m² | 13.3 - 26.2 ft-lb/in² | Average value: 42.2 kJ/m² Grade Count:9 |
|
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..
|
|||