Polymer Property : Izod Impact, Unnotched (ISO) = 30.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP FARADEX NX96302 PC+ABS
LNP* FARADEX* NX96302 is a compound based on PC+ABS resin containing Stainless Steel Fibers.
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature -30.0 °C
14.3 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL V01525 PPE+HIPS
Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature -30.0 °C
14.3 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific)
Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature -30.0 °C
14.3 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL V03550 PPE+HIPS
Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature 23.0 °C
14.3 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem 2212 PEI (Europe-Africa-Middle East)
20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific)
40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East)
40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing.
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
ISO 180
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature -30.0 °C
14.3 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature -30.0 °C
14.3 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East)
VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature 23.0 °C
14.3 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp JF003L PES
LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific)
LNP* Thermocomp* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature 23.0 °C
14.3 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66
LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON MV005SX0 PP (Europe-Africa-Middle East)
LNP* VERTON* MV005SX0 is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized.
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific)
Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL GFN1740V PPE+PS
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature -30.0 °C
14.3 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL GFN1740V PPE+PS
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific)
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature -30.0 °C
14.3 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific)
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Asia Pacific)
PPE+PS blend. 20% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature -30.0 °C
14.3 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Europe-Africa-Middle East)
PPX640 is a 40% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. NSF Standard 61 Compliant (color limited)...
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear
LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature 23.0 °C
14.3 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66 (Europe-Africa-Middle East)
LNP* Stat-kon* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature 23.0 °C
14.3 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp EF006R PEI (Europe-Africa-Middle East)
LNP* Thermocomp* EF006R is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Mold Release.This data was supplied by SABIC-IP for the Europe-A..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
<br>@Temperature 23.0 °C
14.3 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp MF0044E PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MF0044E is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features include: Non-Halogen Flame Retardant, Easy Molding.This data was supplied ..
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
ASTM D256
Tipco Tipcofil® KMX 800 FR - UL94-V0 Flame Retardant, Highly Filled PBT/PC Alloy, with High Heat Stability
Highly Filled, Flame Retardant PBT/PC Alloy, for Injection Molding of "Ceramic Effect" PartsApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacture..
Izod Impact, Unnotched (ISO) 30.0 - 100 kJ/m²
<br>@Temperature -30.0 - -30.0 °C
14.3 - 47.6 ft-lb/in²
<br>@Temperature -22.0 - -22.0 °F
Average value: 57.0 kJ/m² Grade Count:12
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Izod Impact, Unnotched (ISO) 30.0 - 55.0 kJ/m²
14.3 - 26.2 ft-lb/in²
Average value: 39.4 kJ/m² Grade Count:9
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..