Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East)
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® 3412R PC (Europe-Africa-Middle East)
LEXAN 3412R is a high viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat.
Izod Impact, Unnotched (ISO) 35.0 - 100 kJ/m²
16.7 - 47.6 ft-lb/in²
Average value: 58.9 kJ/m² Grade Count:12
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
d.a.m.; ISO 180-1U
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature 23.0 °C
16.7 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180-1U
Lanxess Pocan® BF 4232 HR 901510 PBT, 30% Glass Fiber
PBT, 30% glass fiber, injection molding, flame retardant, hydrolysis stabilizedInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature 23.0 °C
16.7 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180-1U
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral
PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP LCL36 PEEK (Europe-Africa-Middle East)
LNP* LUBRICOMP* LCL36 is a compound based on Polyetheretherketone containing Carbon Fiber , PTFE. Added features of this material include Electrically Conductive, Internally Lubricated.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature 23.0 °C
16.7 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK (Europe-Africa-Middle East)
LNP*LUBRICOMP* LFL36 is a compound based on Polyetheretherketone resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-A..
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP
LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE...
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature -30.0 °C
16.7 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature -30.0 °C
16.7 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be..
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature -30.0 °C
16.7 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM AR9300 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature -30.0 °C
16.7 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM CRS5311 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li..
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM HU2400 PEI
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature 23.0 °C
16.7 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 175 PBT
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature -30.0 °C
16.7 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East)
VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
ISO 180
Solvay Specialty Polymers Ryton® R-4-280BL Polyphenylene Sulfide (PPS), Glass Fiber
Ryton® R-4-280BL 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis..
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific)
Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT..
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature -30.0 °C
16.7 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® V9260CS PET (Asia Pacific)
Color Stable Glass filled PET
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON OEL13I PPS - Linear
LNP* STAT-KON* OEL13I is a compound based on PPS-Linear resin containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: High Impact, Wear Resistant, Electrically Conductive.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP JF004RXP PES (Europe-Africa-Middle East)
LNP* Thermocomp* JF004RXP is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Mold Release.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOTUF MF0049I PP (Europe-Africa-Middle East)
LNP* THERMOTUF* MF0049I is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features include; Flame Retardant, Chemically Coupled.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 4512 PBT+PC (Europe-Africa-Middle East)
10% GF FR PBT/PC Blend
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature 23.0 °C
16.7 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp MF004S PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MF004S is a compound based on Polypropylene resin, containing Glass Fiber. Added features include; Chemically Coupled.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature -30.0 °C
16.7 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180/1U
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA &nbsp;(Unverified Data**)
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal..
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Staramide PFB42U PA6, Glass Fiber/Bead Filled, Injection Molded
Starflam PFB42U is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starflam PX06010 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PX06010 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starglas FF004 HDPE, Glass Fiber Filled
Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Staramide RFM3353EM PA66/6, Glass/Mineral Fiber Reinforced, Injection Molding
Starflam RFM3353EM is a Mineral Filled, Glass Fiber Reinforced Polyamide 66/ Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
<br>@Temperature -30.0 °C
16.7 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific)
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
Copyright © lookpolymers.com All Rights Reserved