Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched (ISO) = 45.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Europe-Africa-Middle East)
This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)  (discontinued **)
Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.
Izod Impact, Unnotched (ISO) 45.0 - 74.0 kJ/m²

@Temperature -30.0 - -30.0 °C
21.4 - 35.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 61.3 kJ/m² Grade Count:3
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
conditioned; ISO 180-1U
Lanxess Durethan® BKV 30 N1 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Asia Pacific)
LNP Lubricomp* KL004 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* Fu..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer (Asia Pacific)
LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UFL36AS is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East)
VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 420HP PBT
30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East)
VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East)
VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East)
VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East)
VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp M10009A PP (Europe-Africa-Middle East)
LNP* STARFLAM* M10009A is a compound based on Polypropylene resin, containing Flame Retardant. Added features include : Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middl..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP UC008H PPA (Asia Pacific)
LNP* THERMOCOMP* UC008H is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP UF00ASW PPA
LNP* Thermocomp* UF00ASW is a compound based on Polyphthalamide (PPA) containing glass fiber. Characteristics of this grade of Heat Stabilized and Hot Water Moldable.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber
Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON KD000EI Acetal Copolymer (Europe-Africa-Middle East)
LNP* Stat-Kon* KD000EI is a compound based on Acetal Copolymer resin containing Carbon Powder. Added features include: Electrically Conductive, Impact Modified.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched (Europe-Africa-Middle East)
LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180/1U
DuPont Performance Polymers Crastin® LW9030 BK851 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 BK851 is a 30% glass fiber reinforced black polybutylene terephthalate blend for injection mol..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180/1U
DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Polyethylene Terephthalate Rynite 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength stiffness and toughness excellent ..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starflam PF0047E PA6, 20% Glass Filled, Injection Molded
Starflam PF0047E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as EXCP4009)Information provided by Polymer Tech..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ASTM D256
Beijing Ranger Chem PBT-201-G15 291 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ASTM D256
BLUESTAR 203G30 PBT, 30% Glass Filled
Typical Applications: Thinner wall partsInformation provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOTUF WF003I PBT (Europe-Africa-Middle East)
LNP* Thermotuf* WF003I BLACK is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact.
Copyright © lookpolymers.com All Rights Reserved