| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC
LNP* LUBRICOMP* DFL36 is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ISO 180/U |
|
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
|
|||
| Izod Impact, Unnotched (ISO) |
55.0
-
60.0
kJ/m² <br>@Temperature -30.0 - -30.0 °C
|
26.2
-
28.6
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 57.5 kJ/m² Grade Count:2 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRILOY RF208 PA 66
LNP LUBRILOY* RF208 is a compound based on Nylon 66 resin containing 40% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant.
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | Type 1; ISO 180 |
|
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry)
Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin..
|
|||
| Izod Impact, Unnotched (ISO) |
55.0
kJ/m² <br>@Temperature -30.0 °C
|
26.2
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East)
VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo..
|
|||
| Izod Impact, Unnotched (ISO) | >= 55.0 kJ/m² | >= 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Europe-Africa-Middle East)
LNP* Stat-Loy* A30009 is a compound based on Acrylonitrile Butadiene resin, containing Proprietary Filler, Flame Retardant. Added features include : Permanent Antistatic, Flame retardant.
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP PF006 PA 6
LNP THERMOCOMP* PF006 is a compound based on Nylon 6 resin containing 30% Glass Fiber.
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP UF008AR PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UF008AR is a compound based on Polyphthalamide resin, containing Glass Fiber. Added features include; Mold Release.
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP UF008AS PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UF008AS is a compound based on Polyphthalamide resin, containing Glass Fiber. Added features include; Mold Release.
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT (Europe-Africa-Middle East)
LNP* Thermotuf* WF006I is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact.
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP VERTON MV00AS PP (Europe-Africa-Middle East)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, heat stabilized
|
|||
| Izod Impact, Unnotched (ISO) |
55.0
kJ/m² <br>@Temperature -30.0 °C
|
26.2
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
|
|||
| Izod Impact, Unnotched (ISO) |
55.0
kJ/m² <br>@Temperature -30.0 °C
|
26.2
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1U |
|
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Asia Pacific)
NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting.
|
|||
| Izod Impact, Unnotched (ISO) |
55.0
kJ/m² <br>@Temperature -30.0 °C
|
26.2
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1U |
|
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Europe-Africa-Middle East)
NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting.
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP IP004Z PA6.12 (Europe-Africa-Middle East)
LNP* LUBRICOMP* IP004Z is a compound based on PA 6/12 resin containing PTFE, Silicone. Added features include : Internally Lubricated, Extrusion grade.
|
|||
| Izod Impact, Unnotched (ISO) |
55.0
kJ/m² <br>@Temperature 23.0 °C
|
26.2
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP Thermocomp RFC16 PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RFC16 is a compound based on PA 66 resin containing Glass Fiber, Carbon Fiber. Added features include: Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
|
|||
| Izod Impact, Unnotched (ISO) |
55.0
kJ/m² <br>@Temperature 23.0 °C
|
26.2
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP Thermotuf PF007IX2 PA 6 (Europe-Africa-Middle East)
LNP * THERMOTUF* PF007IX2 is a compound based on PA 6 resin containing Glass Fiber. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Unnotched (ISO) |
55.0
kJ/m² <br>@Temperature -30.0 °C
|
26.2
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Asia Pacific)
PPE+PS, HDT 125
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 50%RH; ISO 180/1U |
|
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ASTM D256 |
|
Beijing Ranger Chem PBT-201-G25 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ASTM D256 |
|
BLUESTAR 201G25 PBT, 25% Glass Filled
Typical Applications: Energy saving lightingInformation provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ASTM D256 |
|
Beijing Ranger Chem PBT-201-G25 291 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ASTM D256 |
|
Beijing Ranger Chem PBT-201-G25 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ASTM D256 |
|
BLUESTAR 201-G25202 PBT, 25% Glass Filled
Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Unnotched (ISO) |
55.0
kJ/m² <br>@Temperature 23.0 °C
|
26.2
ft-lb/in² <br>@Temperature 73.4 °F
|
80x10x4mm; ISO 180/1U |
|
SYNTHOS Krasten® 336M High Impact Polystyrene
Easy flow grade. Processed by injection moulding of intricate and thin-walled products that enables high production output.Synthos was formerly known as Kaucuk. All information provided by Synthos.
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | DAM; ISO 180/1U |
|
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66
(Unverified Data**)
14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS BK099 is a 14% glass fiber reinforced toughened high flow heat stabilized black polyamide 66 resin. It offers outstanding p..
|
|||
| Izod Impact, Unnotched (ISO) |
55.0
-
67.0
kJ/m² <br>@Temperature -30.0 - -30.0 °C
|
26.2
-
31.9
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 61.0 kJ/m² Grade Count:2 |
|
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
|
|||
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | ASTM D256 |
|
Beijing Ranger Chem PBT-201-G0 211 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||