| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Unnotched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PPS Eco-FR compound
|
|||
| Izod Impact, Unnotched (ISO) | >= 6.00 kJ/m² | >= 2.86 ft-lb/in² | ISO 180/1A |
|
Iran Petrochemical (PCC) Tabriz 4240/1 High Impact Polystyrene
(discontinued **)
Information provided by Iran Petrochemical Commercial Co.
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | DIN 53453 |
|
Ineos Nova S-7600MG Compact Polystyrene Microgranulates
(discontinued **)
High impact polystyrene Microgranulates, having a diameter of 0.8 -1.0 mm, especially useful for compounding and extrusion applications. Due to the very high viscosity and the absence of weakener, ..
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN
LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati..
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP CF008 PS
LNP* THERMOCOMP* CF008 is a compound based on Polystyrene resin containing 40% Glass Fiber.
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP THERMOCOMP AH0400A ABS
LNP* THERMOCOMP* AH0400A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity.
|
|||
| Izod Impact, Unnotched (ISO) |
6.00
kJ/m² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP Thermocomp OF002A PPS
LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Unnotched (ISO) |
6.00
kJ/m² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP Thermocomp OF002A PPS (Asia Pacific)
LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180/1C |
|
Chi Mei Polyrex® PG-22 Polystyrene
TPE compound
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Spec; ISO 180 |
|
Axion Polymers Axpoly® PS01 3003 Enhanced White General Purpose Polystyrene
PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co..
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Spec; ISO 180 |
|
Axion Polymers Axpoly® PS01 3009 Green General Purpose Polystyrene
PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co..
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Spec; ISO 180 |
|
Axion Polymers Axpoly® PS01 Impact Modified Polystyrene
100% post-consumer recycled polymer (recovered from refrigerators)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in a range of co..
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Spec; ISO 180 |
|
Axion Polymers Axpoly® PS02 1000 General Purpose Polystyrene
PS02 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin com..
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 - 16.0 kJ/m² | 2.86 - 7.61 ft-lb/in² | Spec; ISO 180 |
|
Axion Polymers Axpoly® PS02 Impact Modified Polystyrene
100% post-consumer recycled polymer (recovered from television casings)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/gr..
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Spec; ISO 180 |
|
Axion Polymers Axpoly® PS13 1000 Impact Modified Polystyrene
PS13 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS13 range of resin co..
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 - 16.0 kJ/m² | 2.86 - 7.61 ft-lb/in² | Spec; ISO 180 |
|
Axion Polymers Axpoly® PS13 Impact Modified Polystyrene
100% post-consumer recycled polymer (recovered from coat hangers)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/greyCost..
|
|||
| Izod Impact, Unnotched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Spec; ISO 180 |
|
Axion Polymers Axpoly® PS01 3000 General Purpose Polystyrene
PS01 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of custom co..
|
|||
| Izod Impact, Unnotched (ISO) |
6.00
kJ/m² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/U |
|
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F..
|
|||