| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
1.00
kJ/m² <br>@Temperature -30.0 °C
|
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® INP222 ABS
Bulk MMASAN. Provides an economical option for achieving greater melt strength in polymers.
|
|||
| Izod Impact, Notched (ISO) | 1.00 kJ/m² | 0.476 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® INP564 ABS+SAN
SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
|
|||
| Izod Impact, Notched (ISO) |
1.00
kJ/m² <br>@Temperature -30.0 °C
|
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® INP576 ABS+SAN
Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc..
|
|||
| Izod Impact, Notched (ISO) |
1.00
kJ/m² <br>@Temperature -30.0 °C
|
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® INP630 ABS+SAN
INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi..
|
|||
| Izod Impact, Notched (ISO) |
1.00
kJ/m² <br>@Temperature -30.0 °C
|
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® INPBMAT ABS
Cross-linked SAN in styrenic matrix. Provides excellent gloss reduction properties. Maintains original polymer properties such as impact etc. Compatible with various polymer such as PVC and ABS. C..
|
|||
| Izod Impact, Notched (ISO) | 1.00 kJ/m² | 0.476 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® INP581 ABS+SAN
High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for..
|
|||
| Izod Impact, Notched (ISO) |
1.00
kJ/m² <br>@Temperature -30.0 °C
|
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® INP581 ABS+SAN
High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for..
|
|||
| Izod Impact, Notched (ISO) | 1.00 kJ/m² | 0.476 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN
LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati..
|
|||
| Izod Impact, Notched (ISO) | 1.00 - 88.2 kJ/m² | 0.476 - 42.0 ft-lb/in² | Average value: 15.8 kJ/m² Grade Count:56 |
|
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
|
|||
| Izod Impact, Notched (ISO) | 1.00 - 100000 kJ/m² | 0.476 - 47600 ft-lb/in² | Average value: 13.2 kJ/m² Grade Count:40 |
|
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
|
|||
| Izod Impact, Notched (ISO) |
1.00
kJ/m² <br>@Temperature -30.0 °C
|
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4mm, Cut; ISO 180/1A |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1020 PP
SABIC® PPcompound 19T1020 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application..
|
|||
| Izod Impact, Notched (ISO) |
1.00
kJ/m² <br>@Temperature 0.000 °C
|
0.476
ft-lb/in² <br>@Temperature 32.0 °F
|
80*10*4mm, Cut; ISO 180/1A |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1040 PP
SABIC® PPcompound 19T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application..
|
|||
| Izod Impact, Notched (ISO) |
1.00
kJ/m² <br>@Temperature -30.0 °C
|
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4mm, Cut; ISO 180/1A |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1040 PP
SABIC® PPcompound 19T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application..
|
|||
| Izod Impact, Notched (ISO) |
1.00
kJ/m² <br>@Temperature -30.0 °C
|
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4mm, Cut; ISO 180/1A |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 37T1020 PP
SABIC® PPcompound 37T1020 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits high impact and high flow, and is suitable for injection mold..
|
|||
| Izod Impact, Notched (ISO) | >= 1.00 kJ/m² | >= 0.476 ft-lb/in² | DIN 53453 |
|
Schwartz Technical Plastics LAMIGAMID® 1200 Cast Polyamide 12, Dry
Application: sprockets, chain-wheels, pulleys, wheels, slide and seal rings, curve disks, etc.Information provided by Schwartz Technical Plastics GmbH
|
|||
| Izod Impact, Notched (ISO) |
<=
1.00
kJ/m² <br>@Temperature -30.0 °C
|
<=
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
|
|||
| Izod Impact, Notched (ISO) |
<=
1.00
kJ/m² <br>@Temperature -30.0 °C
|
<=
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Asia Pacific)
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
|
|||
| Izod Impact, Notched (ISO) |
<=
1.00
kJ/m² <br>@Temperature -30.0 °C
|
<=
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East)
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
|
|||
| Izod Impact, Notched (ISO) | 1.00 kJ/m² | 0.476 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12
LNP* THERMOCOMP* SF00A is a compound based on Nylon 12 resin containing 50% Glass Fiber.
|
|||
| Izod Impact, Notched (ISO) |
1.00
kJ/m² <br>@Temperature 23.0 °C
|
0.476
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East)
Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) | 1.00 kJ/m² | 0.476 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP QFL32 PA 6/10
LNP* LUBRICOMP* QFL32 is a compound based on Nylon 6/10 containing 10% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant.
|
|||
| Izod Impact, Notched (ISO) | 1.00 kJ/m² | 0.476 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 (Asia Pacific)
Glass filled Nylon 12
|
|||
| Izod Impact, Notched (ISO) | 1.00 kJ/m² | 0.476 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
|
|||
| Izod Impact, Notched (ISO) | 1.00 kJ/m² | 0.476 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT (Asia Pacific)
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
|
|||
| Izod Impact, Notched (ISO) |
1.00
kJ/m² <br>@Temperature -30.0 °C
|
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4mm, Cut; ISO 180/1A |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1020 PP
SABIC® PPcompound 15T1020. This grade is a general purpose, talc filled, heat stabilized polypropylene resin suitable for injection molded applications. The IMDS ID is 16486973.
|
|||
| Izod Impact, Notched (ISO) | 1.00 kJ/m² | 0.476 ft-lb/in² | 80*10*4mm, Cut; ISO 180/1A |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1040 PP
SABIC® PPcompound 15T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound, suitable for injection molding applications. The IMDS ID is 16487994
|
|||
| Izod Impact, Notched (ISO) | 1.00 kJ/m² | 0.476 ft-lb/in² | 80*10*4mm, Cut; ISO 180/1A |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1030 PP
SABIC® PPcompound 19T1030 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding applications...
|
|||
| Izod Impact, Notched (ISO) |
1.00
kJ/m² <br>@Temperature -30.0 °C
|
0.476
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4mm, Cut; ISO 180/1A |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1030 PP
SABIC® PPcompound 19T1030 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding applications...
|
|||
| Izod Impact, Notched (ISO) | 1.00 kJ/m² | 0.476 ft-lb/in² | |
|
Zelfo Technology Zelfo® HG Cellulose Fiber Material
Zelfo® is a high performance bio-based material. Patented fibre technology developed by Zelfo Technology transforms 100% renewable or recycled cellulose fibres and water into self-binding Zelfo mat..
|
|||
| Izod Impact, Notched (ISO) | 1.00 kJ/m² | 0.476 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON ME003S PP
LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized.
|
|||