| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
1.90
ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
|
Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP FARADEX PS003E PA 6
LNP* FARADEX* PS003E is a compound based on Nylon 6 resin containing 15% Stainless Steel. Added features of this material include: EMI/RFI Shielding.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP KONDUIT ITF2B PA 6/12 (Asia Pacific)
LNP* Konduit* ITF2B is a compound based on Nylon 6/12 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature 23.0 °C |
1.90
ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
|
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | Low Temp; DIN 53453 |
|
Ineos Nova S-4400 High Impact Compact Polystyrene
(discontinued **)
Impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection molding of technical parts o..
|
|||
| Izod Impact, Notched (ISO) |
4.00
-
10.0
kJ/m² @Temperature -40.0 - -20.0 °C |
1.90
-
4.76
ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 7.31 kJ/m² Grade Count:4 |
|
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP MG004 PP (Europe-Africa-Middle East)
LNP* Lubricomp* MG004 is a compound based on Polypropylene resin containing Graphite Powder.
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature 23.0 °C |
1.90
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As..
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature 23.0 °C |
1.90
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Lubricomp WBG16 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WBG16 is a compound based on Polybutylene Terephalate resin containing Glass Bead, Graphite.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature 23.0 °C |
1.90
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS
LNP STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This dat..
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature 0.000 °C |
1.90
ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® 325FC PBT (Europe-Africa-Middle East)
Commercial, VALOX 325FC is compliant with food contact regulations. VALOX 325FC is a general purpose, unreinforced PBT injection moulding resin which contains internal mold release. This new 325FC g..
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature -30.0 °C |
1.90
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® 325FC PBT (Europe-Africa-Middle East)
Commercial, VALOX 325FC is compliant with food contact regulations. VALOX 325FC is a general purpose, unreinforced PBT injection moulding resin which contains internal mold release. This new 325FC g..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON WE002 PBT
LNP STAT-KON* WE002 is a compound based on PBT resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature -30.0 °C |
1.90
ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific)
Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP MX06402H PP
LNP* THERMOCOMP* MX06402H is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, Low Extractable.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Asia Pacific)
NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting.
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature -30.0 °C |
1.90
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON RE0029 PA 66
LNP* STAT-KON* RE0029 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature 23.0 °C |
1.90
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12
LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature -30.0 °C |
1.90
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL FE1520PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1520PW resin is a blend of polyphenylene oxide (PPO) and polystyrene (PS) resin that contains 20% glass reinforcement. The resin is suitable for injection molding. Noryl FE1520PW resin has ..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | ASTM D256 |
|
Tipco Tipcolene® FPT 40 NEX - 40% Talc Reinforced Polypropylene Homopolymer, Low MFI
40% Talc Reinforced PP HomopolymerApplications: Sheets, Pipes, ProfilesProcessing: ExtrusionInformation provided by the Manufacturer, Tipco Industries Ltd.,
India.
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | ISO 180 |
|
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80x10x4; ISO 180/1A |
|
Eurostar Staramide BT6 PA6, 30% Mineral Filled, Injection Molded
Staramide BT6 is a 30% Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature -40.0 °C |
1.90
ft-lb/in² @Temperature -40.0 °F |
ISO Test |
|
BASF Ultramid® 8202 HS BK-102 PA6 (Dry)
Ultramid 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose injection molding PA6 exhibiting excellent fluidity for filling thin sections. It possesses ..
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature -40.0 °C |
1.90
ft-lb/in² @Temperature -40.0 °F |
ISO Test |
|
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin..
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature -30.0 °C |
1.90
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen..
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature -30.0 °C |
1.90
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Asia Pacific)
Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen..
|
|||
| Izod Impact, Notched (ISO) |
4.00
kJ/m² @Temperature -30.0 °C |
1.90
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen..
|
|||
| Izod Impact, Notched (ISO) |
4.00
-
8.00
kJ/m² @Temperature -30.0 - 30.0 °C |
1.90
-
3.81
ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 5.63 kJ/m² Grade Count:4 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
|
|||
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON QE002S PA6.10
LNP* STAT-KON* QE002S is a compound based on Nylon 6/10 containing 10% carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive.
|
|||