| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 12.0 - 100000 kJ/m² | 5.71 - 47600 ft-lb/in² | Average value: 110 kJ/m² Grade Count:14 |
|
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
|
|||
| Izod Impact, Notched (ISO) | 1.00 - 100000 kJ/m² | 0.476 - 47600 ft-lb/in² | Average value: 13.2 kJ/m² Grade Count:40 |
|
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
|
|||
| Izod Impact, Notched (ISO) | 2.50 - 100000 kJ/m² | 1.19 - 47600 ft-lb/in² | Average value: 14.6 kJ/m² Grade Count:33 |
|
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
|
|||
| Izod Impact, Notched (ISO) | 5.00 - 100000 kJ/m² | 2.38 - 47600 ft-lb/in² | Average value: 18.1 kJ/m² Grade Count:11 |
|
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| Izod Impact, Notched (ISO) | 3.00 - 100000 kJ/m² | 1.43 - 47600 ft-lb/in² | Average value: 4.20 kJ/m² Grade Count:5 |
|
Overview of materials for Nylon 6, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate..
|
|||
| Izod Impact, Notched (ISO) | 2.50 - 100000 kJ/m² | 1.19 - 47600 ft-lb/in² | Average value: 11.1 kJ/m² Grade Count:19 |
|
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
|
|||
| Izod Impact, Notched (ISO) | 2.50 - 100000 kJ/m² | 1.19 - 47600 ft-lb/in² | Average value: 6.56 kJ/m² Grade Count:10 |
|
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
|
|||