| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | ISO 180 |
|
PolyOne Nymax™ GMF 604 40 UV Black 115 1 X 1 Polyamide 6 (Nylon 6)
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 0.000 °C
|
5.71
ft-lb/in² <br>@Temperature 32.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics GELOY HRA222 ASA+PC (Europe-Africa-Middle East)
GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 0.000 °C
|
5.71
ft-lb/in² <br>@Temperature 32.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Asia Pacific)
Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 263R PC (Europe-Africa-Middle East)
LEXAN 263R is a medium viscosity multi purpose UV stabilized grade and contains release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved.
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HP4R PC (Asia Pacific)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a hig..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® IR 2210 PC (Europe-Africa-Middle East)
PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® ML104R PC (Europe-Africa-Middle East)
LEXAN ML104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatibility inform..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® PC0700 PC (Asia Pacific)
PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® PC1000R PC (Europe-Africa-Middle East)
PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS
Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses.
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 141R PC (Europe-Africa-Middle East)
LEXAN 141R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 141R is available in transparent, translucent and opaque colours.
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 950A PC (Europe-Africa-Middle East)
LEXAN 950A is a high viscosity flame retardant grade, especially suitable for electrical applications.
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | ISO 180/A |
|
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East)
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
|
|||
| Izod Impact, Notched (ISO) |
12.0
-
14.0
kJ/m² <br>@Temperature -30.0 - -30.0 °C
|
5.71
-
6.66
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 13.0 kJ/m² Grade Count:4 |
|
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | ISO 180/1eA |
|
Solvay TECHNYL® A 225F PA66, Conditioned
Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC0703R PC (Europe-Africa-Middle East)
PC0703R resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market.
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP QFP36 PA6.10 (Europe-Africa-Middle East)
LNP* LUBRICOMP* QFP36 is a compound based on PA6.10 resin containg Glass Fiber, PTFE, Silicone. Added features include: Internally Lubricated.
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | ISO 180 |
|
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66
LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI..
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP RF008ESY PA 66
LNP THERMOCOMP* RF008ESY is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | ISO 180/1A |
|
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY
Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used..
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | ISO 180/1A |
|
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, Conditioned
Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph..
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80x10x4; ISO 180/1A |
|
Eurostar Star L POM D36 POM, Injection Molded
Star L POM D36 is Molybdenum Disulfide Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | Conditioned; ISO 180/1A |
|
Addiplast Addinyl A2 E Flame Retardant Nylon 66
Flame retardant, halogen freeInformation provided by Addiplast.
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | ISO 180 |
|
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(disconti
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
|
|||
| Izod Impact, Notched (ISO) |
12.0
-
16.0
kJ/m² <br>@Thickness 3.20 - 3.20 mm
|
5.71
-
7.61
ft-lb/in² <br>@Thickness 0.126 - 0.126 in
|
Average value: 15.1 kJ/m² Grade Count:36 |
|
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature 23.0 °C
|
5.71
ft-lb/in² <br>@Temperature 73.4 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont ..
|
|||
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP 9X11427
LNP* THERMOCOMP* 9X11427 is a compound based on Miscellanbeous resin containing 40% specialty glass filled TP alloy. Added features of this grade include: Ultra-Stiff Toughness, Improved Impact, G..
|
|||
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 943 PC (Europe-Africa-Middle East)
LEXAN 943 is a medium viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications.
|
|||