| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature -30.0 °C
|
0.952
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
|
|||
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature -30.0 °C
|
0.952
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® INP563 ABS+SAN
SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PPS Eco-FR compound
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS
LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Izod Impact, Notched (ISO) |
2.00
-
2.00
kJ/m² <br>@Temperature -30.0 - -30.0 °C
|
0.952
-
0.952
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 2.58 kJ/m² Grade Count:1 |
|
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
|
|||
| Izod Impact, Notched (ISO) |
2.00
-
16.0
kJ/m² <br>@Temperature -30.0 - -30.0 °C
|
0.952
-
7.61
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 4.25 kJ/m² Grade Count:24 |
|
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12
LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant.
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP OL003A PPS - Branched
LNP* LUBRICOMP* OL003A is a compound based on PPS - Branched resin containing 15% PTFE. Added features of this grade are: Wear Resistant.
|
|||
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature -30.0 °C
|
0.952
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4mm, Cut; ISO 180/1A |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1040 PP
SABIC® PPcompound 55T1040 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact and high rigidity, and is suitable for injec..
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP RL0049S PA 66
LNP LUBRICOMP* RL0049S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Flame Retardant, Heat Stabilized, Wear Resistant.
|
|||
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature -30.0 °C
|
0.952
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.
|
|||
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature -30.0 °C
|
0.952
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend (Asia Pacific)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.
|
|||
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature -30.0 °C
|
0.952
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend (Asia Pacific)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East)
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature 23.0 °C
|
0.952
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® 175 PBT
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature -30.0 °C
|
0.952
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific)
Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +..
|
|||
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature -30.0 °C
|
0.952
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® IQ325HP PBT (Asia Pacific)
FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications.
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON FD000 PE
LNP* STAT-KON* FD000 is an unfilled Polyethylene. Added feature of this grade is: Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature -30.0 °C
|
0.952
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON MX01739C PP
LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
|
|||
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature -30.0 °C
|
0.952
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East)
FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications.
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP MX89510 PP
LNP* THERMOCOMP* MX89510 is a compound based on Polypropylene resin containing Proprietary Filler(s).
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | ASTM D256 |
|
Tipco Tipcolite® TG 613 Phenolic Compound, Mineral & Wood Flour, Soft Flow & Good Surface Finish
Soft Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: General PurposeProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India...
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80x10x4; ISO 180/1A |
|
Eurostar Starpylen HZ 80E7 HDPE, Injection Molding
Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | ISO 180/1A |
|
Chi Mei Polyrex® PG-80N Polystyrene
High strength
|
|||
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature -30.0 °C
|
0.952
ft-lb/in² <br>@Temperature -22.0 °F
|
50%RH; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info..
|
|||
| Izod Impact, Notched (ISO) |
2.00
kJ/m² <br>@Temperature 23.0 °C
|
0.952
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific)
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa..
|
|||
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON OE002 PPS - LINEAR
LNP* STAT-KON* OE002 is a compound based on PPS - Linear resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) | 2.00 - 48.0 kJ/m² | 0.952 - 22.8 ft-lb/in² | Average value: 18.1 kJ/m² Grade Count:79 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded