Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 28.6 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.50 - 60.0 kJ/m²
1.67 - 28.6 ft-lb/in²
Average value: 8.52 kJ/m² Grade Count:75
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Izod Impact, Notched (ISO) 3.00 - 60.0 kJ/m²

@Temperature -40.0 - 0.000 °C
1.43 - 28.6 ft-lb/in²

@Temperature -40.0 - 32.0 °F
Average value: 10.7 kJ/m² Grade Count:54
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched (ISO) 3.50 - 60.0 kJ/m²
1.67 - 28.6 ft-lb/in²
Average value: 17.0 kJ/m² Grade Count:27
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Izod Impact, Notched (ISO) 5.00 - 60.0 kJ/m²
2.38 - 28.6 ft-lb/in²
Average value: 26.9 kJ/m² Grade Count:12
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Izod Impact, Notched (ISO) 60.0 - 60.0 kJ/m²

@Temperature -20.0 - -20.0 °C
28.6 - 28.6 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 15.1 kJ/m² Grade Count:3
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Notched (ISO) 2.00 - 60.0 kJ/m²
0.952 - 28.6 ft-lb/in²
Average value: 7.59 kJ/m² Grade Count:44
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Copyright © lookpolymers.com All Rights Reserved