Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics EXTEM UH1006 TPI Blend
High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha..
Izod Impact, Notched (ISO) 9.00 kJ/m²
<br>@Temperature -30.0 °C
4.28 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
Izod Impact, Notched (ISO) 9.00 kJ/m²
<br>@Temperature -30.0 °C
4.28 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East)
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS
LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Izod Impact, Notched (ISO) 9.00 kJ/m²
<br>@Temperature -30.0 °C
4.28 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics GELOY XP7550 ASA+PC
Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow.
Izod Impact, Notched (ISO) 9.00 kJ/m²
<br>@Temperature -30.0 °C
4.28 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
Izod Impact, Notched (ISO) 9.00 kJ/m²
<br>@Temperature -30.0 °C
4.28 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER
Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
Izod Impact, Notched (ISO) 9.00 - 30.0 kJ/m²
4.28 - 14.3 ft-lb/in²
Average value: 13.7 kJ/m² Grade Count:6
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Izod Impact, Notched (ISO) 9.00 kJ/m²
<br>@Temperature -20.0 °C
4.28 ft-lb/in²
<br>@Temperature -4.00 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL PX9406P PPE+HIPS (Asia Pacific)
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 125dc HDT. UL94 V-0 rated. Electrical applications.
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP RFP36S PA 66
LNP* LUBRICOMP* RFP36S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Heat Stabilized.
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Asia Pacific)
LNP LUBRICOMP* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP ZFL24 PPE+PS
LNP* LUBRICOMP* ZFL24 is a compound based on PPE+PS resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is: Wear Resistant.
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP STAT-KON DD0009P PC (Asia Pacific)
LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Europe-Africa-Middle East)
LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Izod Impact, Notched (ISO) 9.00 kJ/m²
<br>@Temperature 23.0 °C
4.28 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East)
High flow Ultem for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® 830F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications
Izod Impact, Notched (ISO) 9.00 kJ/m²
<br>@Temperature -30.0 °C
4.28 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific)
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.
Izod Impact, Notched (ISO) 9.00 kJ/m²
<br>@Temperature 23.0 °C
4.28 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermocomp EF008EXP PEI (Europe-Africa-Middle East)
LNP* Thermocomp* EF008EXP is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SABIC-IP ..
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Chemically Coupled.
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA
LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing 40% Glass Fiber. Added feature of this grade is: Healthcare.
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66
LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Izod Impact, Notched (ISO) 9.00 kJ/m²
<br>@Temperature -30.0 °C
4.28 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East)
Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating ..
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180/1A
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, Conditioned
Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding...
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180
Tisan TISREN® Flame Retardant (V0) Polystyrene
TISREN has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimensio..
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180A
Chevron Phillips Xtel® XE5030BL Polyphenylene Sulfide Alloy
Xtel® XE5030BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.Information provided by Chevr..
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66 &nbsp;(Unverified Data**)
13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL is a 13% glass fiber reinforced heat stabilized lubricated slightly toughened polyamide 66 for injection molding. It has im..
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
50%RH; ISO 180/1A
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6 &nbsp;(Unverified Data**)
40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly..
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ASTM D256
Beijing Ranger Chem PBT 403 M-G15 Heat Resistant and Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
1A; ISO 180
Azoty Tarnow™ TARNOFORM 200 POM
This material is a standard extrusion grade, also could be used for injection molding of low shape complexity details.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOTUF WF003I PBT (Europe-Africa-Middle East)
LNP* Thermotuf* WF003I BLACK is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact.
Copyright © lookpolymers.com All Rights Reserved