Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.50 - 70.0 kJ/m²
2.14 - 33.3 ft-lb/in²
Average value: 13.0 kJ/m² Grade Count:88
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Izod Impact, Notched (ISO) 4.50 kJ/m²
<br>@Temperature 23.0 °C
2.14 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/1A
DuPont Performance Polymers Crastin® S600F20 NC010 PBT &nbsp;(Unverified Data**)
Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180/A
Victrex® HT™ P22 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact compliantInfo..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180/A
Victrex® HT™ P22PF Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, easy flow, FDA food contact compliantInfo..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
Low Temp; DIN 53453
Ineos Nova S-3500MG Compact Polystyrene Microgranulates &nbsp;(discontinued **)
Very easy flowing medium impact polystyrene Microgranulates, having a diameter of 0.8 - 1.0 mm and a very large specific surface areas. This grade is especially designed for use in compounding and ..
Izod Impact, Notched (ISO) 4.50 kJ/m²
<br>@Temperature 23.0 °C
2.14 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/A
Victrex® PEEK 150P Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact complian..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180/A
Victrex® PEEK 150PF Easy Flow
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, easy flow, FDA food contact compliant, ..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
Result based on similar products; ISO 180/A
Victrex® PEEK 150UF10 Polyetheretherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for composite manufacture, easy flow, FDA food contact compliant..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180
Iran Petrochemical (PCC) Moplen EP1 X 35 AF Polypropylene
Moplen EP1 X 35 AF is a slightly modified random copolymer for the production of cast and water-quenched blown film. It is formulated with a slip and antiblock package and exhibits excellent antist..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180/1eA
Solvay TECHNYL® C 216 PA6, DRY
Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180/1A
Solvay TECHNYL® A 208F PA66, DRY
Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180
Polyram PlusTek PA301G2 Nylon 6.6 for Injection Molding, 10% Glass Fiber Reinforced, Heat Stabilized
Heat stabilized, 10% Glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 4.50 kJ/m²
<br>@Temperature -20.0 °C
2.14 ft-lb/in²
<br>@Temperature -4.00 °F
ISO 179
Total PPC 12712 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180/1A
DuPont Performance Polymers Crastin® FG6129 NC010 Polybutylene Terephthalate (PBT) &nbsp;(Unverified Data**)&lt
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6129 NC010 is an unreinforced high viscosity polybutylene..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180/1A
DuPont Performance Polymers Sorona® 3301 BK001 Polytrimethylene Terephthalate (PTT) &nbsp;(Unverified Data**)&l
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight w..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180/1A
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT) &nbsp;(Unverified Data**)&l
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with su..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180/1A
DuPont Performance Polymers Sorona® FG3301 NC010 Polytrimethylene Terephthalate (PTT) &nbsp;(Unverified Data**)
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Developed for Food Contact Applications Sorona FG3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renew..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® 70G13HS1L BK031 Nylon 66 &nbsp;(Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L BK031 is a 13% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
80x10x4; ISO 179/1eA
Eurostar Staramide RF006S-GY9A121 PA66, 30% Glass Fiber Filled, Injection Molded
Staramide RF006S-GY9A121 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612 &nbsp;(Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 4.50 kJ/m²
<br>@Temperature -30.0 °C
2.14 ft-lb/in²
<br>@Temperature -22.0 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612 &nbsp;(Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612 &nbsp;(Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 4.50 kJ/m²
<br>@Temperature -30.0 °C
2.14 ft-lb/in²
<br>@Temperature -22.0 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612 &nbsp;(Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66 &nbsp;(Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
Izod Impact, Notched (ISO) 4.50 kJ/m²
<br>@Temperature -40.0 °C
2.14 ft-lb/in²
<br>@Temperature -40.0 °F
ISO Test
BASF Ultramid® B3EG3 BK00564 15% Glass Filled PA6 (Dry)
Ultramid B3EG3 BK00564 is a 15% glass fiber reinforced, pigmented black injection molding PA6 grade for housings with enhanced impact resistance.