Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Asia Pacific)
Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1...
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1...
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER
LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an..
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER
Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. ..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HP2R PC (Europe-Africa-Middle East)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a hi..
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® 144R PC
UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer ..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HP3REU PC (Europe-Africa-Middle East)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold ..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® XHT1141 PC (Asia Pacific)
XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors.
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
<= 4.76 ft-lb/in²
d.a.m.; ISO 180-1A
Lanxess Durethan® BKV 15 DUS008 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 15% glass fibers, injection moldingInformation provided by LANXESS.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4mm, Cut; ISO 180/1A
SABIC Innovative Plastics SABIC PPCOMPOUND G3240U PP
SABIC® PPcompound G3240U is a general purpose, 40% glass filled, chemically coupled, heat stabilized and UV stabilized homopolymer polypropylene compound. The IMDS ID is 209768078.
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 (Asia Pacific)
LNP Lubricomp is a compound based on PA66 resin containing glass fiber, PTFE. It is an internally lubricated compound that provide excellent chemical resistance, strength and wear/friction propertie..
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WFP36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Silicone.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP STAT-LOY KX05015 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Stat-Loy* KX05015 is a compound based on Acetal Copolymer resin containing Antistat. Added features include permanent Anti-Static.
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East)
PPX630 is a 30% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. Generic identification acc. ISO11469: PP+PP..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermocomp EF006R PEI (Europe-Africa-Middle East)
LNP* Thermocomp* EF006R is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Mold Release.This data was supplied by SABIC-IP for the Europe-A..
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180
DSM Fibre Intermediates Nyrim® 2025 (Wollastocoat®), Conditioned
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80x10x4; ISO 180/1A
Eurostar Star C BX6088 ABS, 20% Carbon Filled, Injection Molding
Star C BX06008 is a 20% Carbon Fiber Reinforced ABS Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180/1A
Total Lacqrene® 4801 &nbsp;(discontinued **)
LACQRENE® 4801 is an easy flowing, high impact polystyrene for injection molding. The very good processing characteristics of this grade allows for the production of thin articles with long flow p..
Izod Impact, Notched (ISO) 10.0 kJ/m²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer
Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based ..
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Europe-Africa-Middle East)
LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber.