Polymer Property : Izod Impact, Notched (ISO) = 47600 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 12.0 - 100000 kJ/m²
5.71 - 47600 ft-lb/in²
Average value: 110 kJ/m² Grade Count:14
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Izod Impact, Notched (ISO) 1.00 - 100000 kJ/m²
0.476 - 47600 ft-lb/in²
Average value: 13.2 kJ/m² Grade Count:40
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Izod Impact, Notched (ISO) 2.50 - 100000 kJ/m²
1.19 - 47600 ft-lb/in²
Average value: 14.6 kJ/m² Grade Count:33
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Izod Impact, Notched (ISO) 5.00 - 100000 kJ/m²
2.38 - 47600 ft-lb/in²
Average value: 18.1 kJ/m² Grade Count:11
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Izod Impact, Notched (ISO) 3.00 - 100000 kJ/m²
1.43 - 47600 ft-lb/in²
Average value: 4.20 kJ/m² Grade Count:5
Overview of materials for Nylon 6, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate..
Izod Impact, Notched (ISO) 2.50 - 100000 kJ/m²
1.19 - 47600 ft-lb/in²
Average value: 11.1 kJ/m² Grade Count:19
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Izod Impact, Notched (ISO) 2.50 - 100000 kJ/m²
1.19 - 47600 ft-lb/in²
Average value: 6.56 kJ/m² Grade Count:10
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..