| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP COLORCOMP EX12304C PEI (Asia Pacific)
LNP* Colorcomp* EX12304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS technol..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Faradex ES003DE PEI
LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific)
LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant.
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON AX01706 ABS
LNP* STAT-KON* AX01706 is a compound based on ABS containing proprietary fillers. Added feature of this grade is: Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON ZE0039 MODIFIED POLYPHENYLENE (Asia Pacific)
LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Stat-kon ZX05009 PPE+PS (Europe-Africa-Middle East)
LNP* Stat-kon* ZX05009 is a compound based on PPE+PS Blend resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -10.0 °C
|
2.38
ft-lb/in² <br>@Temperature 14.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific)
PC+Polyester, UV Stabilized, Transparent
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP OE004A PPS - BRANCHED (Europe-Africa-Middle East)
LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive. (only Black is UL listed)
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics ULTEM AUT200 PEI
Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperat..
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer
LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East)
10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP DC0049XF PC
LNP* THERMOCOMP* DC0049XF is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East)
LNP* THERMOCOMP* OC004 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180 |
|
Polyram PlusTek PA201 Nylon 66 for Extrusion
High viscosity Nylon 66 for extrusion applications.Information provided by Polyram.
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ASTM D256 |
|
Tipco Tipcolene® PPH-OIT - Unfilled Polypropylene Homopolymer Compound with Copper Inhibitor (Metal Deactivator)
PP Homopolymer with Copper Inhibitor (Metal De-activator)Applications: Automotives & ElectricalProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India.
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180 |
|
Total Lumicene® MR60MC2 Metallocene Random Copolymer Polypropylene, Injection Molding
Lumicene® MR60MC2 is a metallocene random copolymer with a melt flow index of 60 g/10 min for injection molding. Lumicene® MR60MC2 differs from standard random copolymers by its molding reproducib..
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ASTM D256 |
|
Tipco Tipcolene® PP-LTHA - Unfilled Polypropylene Homopolymer with Long Term Heat Aging Stability
PP Homopolymer with Long Term Heat Aging StabilityApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India.
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80x10x4; ISO 180/1A |
|
Eurostar Starglas OC004 PPS, 20% Carbon Filled, Injection Molded
Starglas OC004 is a 20% Carbon Fiber Reinforced PPS Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180/1A |
|
Addiplast Addinyl A2 ZV15 Nylon 66, 15% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180/A |
|
BASF Ultramid® B3S HP PA6 (Dry)
Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/A |
|
BASF Ultramid® B3S HP PA6 (Dry)
Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing
|
|||
| Izod Impact, Notched (ISO) | 5.00 - 6.00 kJ/m² | 2.38 - 2.86 ft-lb/in² | Average value: 5.75 kJ/m² Grade Count:4 |
|
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max..
|
|||
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180-93 |
|
Wellman Wellamid® 22L-NBK1/WE-1434 Nylon 66, Engineering Grade
All information provided by Wellman Engineered Resins.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics GELOY XP4025 ASA+PC
Available in a wide range of colors and is recommended for unpainted exterior applications.
|
|||