Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 13.0 kJ/m²
<br>@Thickness 4.00 mm,<br> Temperature 23.0 °C
6.19 ft-lb/in²
<br>@Thickness 0.157 in,<br> Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® ESD 5500 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5500 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5500 can be injectio..
Izod Impact, Notched (ISO) 13.0 kJ/m²
<br>@Temperature -30.0 °C
6.19 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP COLORCOMP D1000P PC
LNP* COLORCOMP* D1000P is an unfilled Polycarbonate. Added feature of this grade is: Exceptional Processing.
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC (Asia Pacific)
LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC
LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated.
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC
LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated.
Izod Impact, Notched (ISO) 13.0 - 13.0 kJ/m²
<br>@Temperature -30.0 - -30.0 °C
6.19 - 6.19 ft-lb/in²
<br>@Temperature -22.0 - -22.0 °F
Average value: 13.0 kJ/m² Grade Count:1
Overview of materials for Nylon 612, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/1eA
Solvay TECHNYL® A 218 V35 Black 34 NG PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218 V35 Black 34 NG is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/1eA
Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, DRY
Description: TECHNYL STAR Polyamide, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Europe and North America ..
Izod Impact, Notched (ISO) 13.0 kJ/m²
<br>@Temperature -30.0 °C
6.19 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East)
VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin.
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/A
Styrolution PS 495F HIPS
Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection..
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP RF008H PA 66
LNP* THERMOCOMP* RF008H is a compound based on Nylon 66 containing 40% Glass Fiber. Added feature of this grade is: Healthcare.
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP RF00AS PA 66
LNP THERMOCOMP* RF00AS is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Notched (ISO) 13.0 kJ/m²
<br>@Temperature 23.0 °C
6.19 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermotuf R1000IX2 PA6.6 (Europe-Africa-Middle East)
LNP* THERMOTUF* R1000IX2 is a compound based on PA 66 resin, containing Impact Modifier. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi..
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP PC006 PA 6 (Europe-Africa-Middle East)
LNP* Thermocomp* PC006 is a compound based on Nylon 6 resin containing Carbon Fiber.
Izod Impact, Notched (ISO) 13.0 kJ/m²
<br>@Temperature 23.0 °C
6.19 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermocomp RF007S PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RF007S is a compound based on PA 66 resin containing Glass Fiber . Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi..
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/1A
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, Conditioned
Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and..
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180
Tisan TISAKRIL® Flame Retardant (V0) ABS
TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens..
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180-93
Wellman Wellamid® GFX1717-BK1 Nylon 66, 43% Glass Fiber Reinforced, Silicone Lubricated
All information provided by Wellman Engineered Resins.
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
Low Temp; ISO 180/1eA
Lubrizol ESTALOC® T514 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80x10x4; ISO 180/1A
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding
Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 13.0 kJ/m²
<br>@Temperature 23.0 °C
6.19 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/1A
DuPont Performance Polymers Rynite® 408 BK515 PET
Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info..
Izod Impact, Notched (ISO) 13.0 kJ/m²
<br>@Temperature 23.0 °C
6.19 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecomid® NA40 KC50 BK111 PA6.6, 50% glass/carbon fiber reinforced, black
Information provided by Eurotec®
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/1A
Addiplast Addinyl A2 ZV40 Nylon 66, 40% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Izod Impact, Notched (ISO) 13.0 kJ/m²
<br>@Temperature -25.0 °C
6.19 ft-lb/in²
<br>@Temperature -13.0 °F
ISO 179/1eA
BASF Ultrason S 3010 PSU
Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655.
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOTUF VX99810 Super Tough Nylon
Super Tough Nylon, Proprietary Filler(s),
Izod Impact, Notched (ISO) 13.0 kJ/m²
<br>@Temperature -30.0 °C
6.19 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East)
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
Izod Impact, Notched (ISO) 13.0 kJ/m²
<br>@Temperature -30.0 °C
6.19 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific)
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
Copyright © lookpolymers.com All Rights Reserved