| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -30.0 °C
|
6.66
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -30.0 °C
|
6.66
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® LUX2010T_ PC (Europe-Africa-Middle East)
Global grade. LEXAN LUX2010T is an injection moulding grade especially designed for manufacturing optical parts requiring excellent flow properties combined with very high transmission and color sta..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® OQ1022 PC (Europe-Africa-Middle East)
Standard Flow OQ Resin
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP FARADEX DS0036IR PC (Europe-Africa-Middle East)
LNP* FARADEX* DS0036IR is a compound based on Polycarbonate resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Improved Paintability, Non-Brominated & Non-Chlorinated F..
|
|||
| Izod Impact, Notched (ISO) |
14.0
-
16.0
kJ/m² <br>@Thickness 3.20 - 3.20 mm
|
6.66
-
7.61
ft-lb/in² <br>@Thickness 0.126 - 0.126 in
|
Average value: 17.5 kJ/m² Grade Count:4 |
|
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
|
|||
| Izod Impact, Notched (ISO) | 14.0 - 95.0 kJ/m² | 6.66 - 45.2 ft-lb/in² | Average value: 68.0 kJ/m² Grade Count:3 |
|
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180 |
|
Iran Petrochemical (PCC) EP-T 30 R Polypropylene
The grade is a medium flow heterophasic the copolymer mainly designed for injection molding application.Application: containers, buckets, pails, crates and also used for automotive parts.Informatio..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP DX09410H PC
LNP* LUBRICOMP* DX09410H is a compound based on Polycarbonate resin containing Proprietary FIllers. Added features of this grade include: Healthcare, Wear Resistant.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180 |
|
Solvay Technyl® A218V43 43% Glass Filled, Heat Stabilized Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific)
LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC (Europe-Africa-Middle East)
LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing Glass Fiber.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC
LNP THERMOCOMP* DF004ER is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. Mold Release.
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature 23.0 °C
|
6.66
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Thermocomp DF0069E PC (Asia Pacific)
LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA 6/12
LNP THERMOCOMP* IF006 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber.
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -30.0 °C
|
6.66
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Asia Pacific)
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific)
Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP DF008 PC
LNP THERMOCOMP* DF008 is a compound based on Polycarbonate resin containing 40% Glass Fiber.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP RX99732C PA 66
LNP* Thermocomp* PDX-R-99732 is a Nylon 6/6 with proprietary fillers.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180 |
|
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ASTM D256 |
|
Tipco Tipcolene® SEB 300 M - 30% Chemically Coupled Glass Fibers & Mineral Polypropylene Homopolymer
30% Mineral + Glass Reinforced, PP Homopolymer for Automobile Engine PartsApplications: Automotive Engine PartsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries..
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -30.0 °C
|
6.66
ft-lb/in² <br>@Temperature -22.0 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**)
33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf..
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -40.0 °C
|
6.66
ft-lb/in² <br>@Temperature -40.0 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**)
43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information..
|
|||
| Izod Impact, Notched (ISO) |
14.0
kJ/m² <br>@Temperature -30.0 °C
|
6.66
ft-lb/in² <br>@Temperature -22.0 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide ..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180/1A |
|
Addiplast Addilene J 310 Polypropylene Copolymer
UnreinforcedInformation provided by Addiplast.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO Test |
|
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Conditioned)
Ultramid 7423-2 NF3001 is an impact modified, 13% glass reinforced, heat stabilized injection molding PA6/6.
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 3146 |
|
BASF Ultramid® 8234G HS BK 102 44% Glass Filled PA6 (Dry)
Description Ultramid 8234G HS BK-102 is heat stabilized, pigmented black, 44% glass reinforced PA6 injection molding compound offering the highest level of strength, stiffness, high temperature perf..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO Test |
|
BASF Ultramid® 8253 HS BK-102 PA6 (Dry)
Ultramid 8253 HS BK-102 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying leve..
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ASTM D256 |
|
BLUESTAR LXS 314 G10 PPE-HIPS, 10% Glass Filled
Typical Applications: Water industrial partsInformation provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched (ISO) | 14.0 kJ/m² | 6.66 ft-lb/in² | ISO 180 |
|
Polyram RamOfin PPC104 Polypropylene Copolymer
Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram.
|
|||