| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 1173X PC Copolymer (Europe-Africa-Middle East)
Lexan* 1173X polycarbonate (PC) resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-30 C) ductility in combination with high flow characteristics an..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 121R PC (Asia Pacific)
Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release.
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 123X PC Copolymer
Improved flow PC with excellent processability and mold release.
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 223R PC (Asia Pacific)
17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized.
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 915R PC (Europe-Africa-Middle East)
Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties...
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 916R PC (Europe-Africa-Middle East)
Lexan* 916R Polycarbonate (PC) resin is a low viscosity, non-filled, injection molding grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating at 0.8 mm properties. Lexan* ..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 9931X PC (Europe-Africa-Middle East)
Lexan* 9931X is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, extreme low temperatu..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer
Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Asia Pacific)
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXD121R PC (Europe-Africa-Middle East)
LEXAN FXD121R is a transparent/translucent low viscosity grade for light diffusion special effects. Color package may affect performance.
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXE121R PC (Europe-Africa-Middle East)
LEXAN FXE121R is a transparent/translucent low viscosity grade for special effects colors with a fluorescent appearance. Color package may affect performance.
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Asia Pacific)
Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer
Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® LS1 PC (Europe-Africa-Middle East)
LEXAN LS1 is a low viscosity injection moulding grade especially designed for manufacturing complex parts requiring easy flow properties combined with high optical requirements.
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® LUX2180T_ PC (Europe-Africa-Middle East)
Global grade. LEXAN LUX2180T is an injection moulding grade especially designed for manufacturing optical parts requiring easy flow properties combined with very high transmission and color stabilit..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® ML3290 PC (Europe-Africa-Middle East)
LEXAN ML3290 is a high viscosity flame retardant UV stabilized grade especially developed for the extrusion of complex sheet and profiles. LEXAN ML3290 is used in applications where a combination of..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® PC2200R PC (Asia Pacific)
PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® PC2200R PC (Europe-Africa-Middle East)
PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East)
PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific)
LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | ISO Test |
|
Styrolution Terblend® N NM-11 ABS/PA6 (Dry)
Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | pb; ISO 180 |
|
A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact..
|
|||
| Izod Impact, Notched (ISO) |
65.0
kJ/m² <br>@Thickness >=5.00 mm
|
30.9
ft-lb/in² <br>@Thickness >=0.197 in
|
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
|
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | DAM; Partial; ISO 180/1A |
|
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610
(Unverified Data**)
Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient..
|
|||
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP