Polymer Property : Four Ball Extreme Pressure, Weld Load = 551 lb (mass) Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
Welding Load; IP 239
Solvay Specialty Polymers FOMBLIN® LC08 PFPE Lubricant
FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
ExxonMobil 0 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
ExxonMobil 100 Mobil Aviation Grease SHC
Mobil Aviation Grease SHC 100 is a supreme performance synthetic grease which combines the unique features of a polyalphaolefin (PAO) synthetic base fluid with those of a high quality lithium comple..
Four Ball Extreme Pressure, Weld Load >= 250 kg
>= 551 lb (mass)
ASTM D2596
ExxonMobil 100 Special Mobiltemp SHC Series
Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base ..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2783
ExxonMobil 150 Mobilgear SHC Series
The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2783
ExxonMobil 1500 Mobilgear SHC Series
The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
ExxonMobil 2 Mobilith AW Series
The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
ExxonMobil 23 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2783
ExxonMobil 27 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2783
ExxonMobil 32 Mobil Mist Lube Series
Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2783
ExxonMobil Spartan EP 320
Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2783
ExxonMobil Spartan EP 68
Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
ExxonMobil 460 Mobilith SHC PM
Mobilith SHC PM greases are supreme performance products designed specifically for severe paper machine applications, including extreme temperature environments and exposure to different qualities o..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ConocoPhillips Syncon® HP Synthetic Grease NLGI No. 1
Description: Conoco Syncon HP Synthetic Grease is a high-quality, synthetic polyalphaolefin (PAO) lithium grease developed to provide exceptional protection and corrosion resistance for bearings and..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
Chesterton 622 White Grease
Description: Chesterton® 622 White Grease is a pure mineral oil grease with PTFE added designed for applications where a clean, nonstaining, food grade lubricant is required. It is a superior, mult..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
ELM® SoyLube® All Purpose Lubricant and Penetrating Oil
Description: SoyLube All Purpose Lubricant and Penetrating Oil is a high performance, biodegradable penetrant and lubricating oil for general purpose use. Formulated with the best optimized USA-gro..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ChevronTexaco Novatex® EP NLGI Grade 000
Texaco Novatex EP are water resistant, extreme pressure greases. They are manufactured using highly refined, select high viscosity index base oils, a calcium soap, and a specifically selected addit..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
ExxonMobil 0 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
ExxonMobil 100 Mobil Aviation Grease SHC
Mobil Aviation Grease SHC 100 is a supreme performance synthetic grease which combines the unique features of a polyalphaolefin (PAO) synthetic base fluid with those of a high quality lithium comple..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
ExxonMobil 3 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2783
ExxonMobil 320 Mobilgear SHC Series
The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2783
ExxonMobil 626 Mobilgear 600 Series
The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives ..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ConocoPhillips 320 Gear Oil AGMA Lubricant No. 6 EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ConocoPhillips 460M Gear Oil AGMA Lubricant No.7EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
ExxonMobil 2 Mobilith AW Series
The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
ExxonMobil 23 Mobilux EP
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ConocoPhillips 1000 Gear Oil AGMA Lubricant No. 8AEP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ConocoPhillips 2 Bentone Grease NLGI No. 2
Description: Conoco Bentone Grease is a high-quality, smooth-textured, clay based grease developed for heavy-duty industrial machinery operating at very high temperatures. Unlike conventional soap-b..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ConocoPhillips Hydroclear® 320 6 EP gear Oil
Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary addi..
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
ExxonMobil Mobil 1 Synthetic Grease
Mobil 1 Synthetic Grease is an NLGI No 2 high-performance grease which combines a synthetic base fluid with a lithium complex soap thickener. The thickener system provides a high dropping point, whi..
Copyright © lookpolymers.com All Rights Reserved